ICP-PECVD (Unaxis VLR): Difference between revisions
(link to Wafer Coating Process Traveler + Recipes page) |
|||
Line 31: | Line 31: | ||
*[http://wiki.nanotech.ucsb.edu/wiki/images/1/1f/Unaxis_PM3_Web_Operational_Procedure_3-27-14.pdf Operating Instructions] |
*[http://wiki.nanotech.ucsb.edu/wiki/images/1/1f/Unaxis_PM3_Web_Operational_Procedure_3-27-14.pdf Operating Instructions] |
||
*[https://wiki.nanotech.ucsb.edu/w/images/a/ab/Unaxis_SOP_3-27-2020.pdf Wafer Coating Process Traveler] |
*[https://wiki.nanotech.ucsb.edu/w/images/a/ab/Unaxis_SOP_3-27-2020.pdf Wafer Coating Process Traveler] |
||
Revision as of 19:00, 30 March 2020
|
About
This system is configured as an ICP PECVD deposition tool with 1000 W ICP power, 600 W RF substrate power, and 50°C-350°C operation. This chamber has 100% SiH4, N2, O2, and Ar for gas sources. The high density PECVD produces a more dense, higher quality SiO2 and Si3N4, as compared with conventional PECVD. With the high density plasma, deposition of high quality films can be deposited as low as 50°C for processes requiring lower temperatures. Stress compensation for silicon nitride is characterized.
Cluster Configuration
A Deposition and Etch chamber are both attached to the same loadlock, allowing etching and deposition without breaking vacuum. Each chamber can be scheduled separately on SignupMonkey.
- PM3: ICP-PECVD Deposition (this page)
- PM1: ICP Etch (Unaxis VLR)
Detailed Specifications
- 1000W ICP source, 600W RF Sample Bias Power Supply
- 50 - 350°C sample temperature
- 100% SiH4, Ar, N2, O2
- Multiple 4” diameter wafer capable system
- Pieces possible by mounting or placing on 4 ” wafer
Documentation
Recipes
You can find recipes for this tool on the Wiki > Recipes > PECVD Recipes page