Wafer Coating Process Traveler: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
Biljana (talk | contribs)
Replaced content with "There are three standard recipes : STD SiO2, STD Nitride2, and STD LS Nitride2 at 300C. Instructions bellow explain how to run each of the recipes ( seasoning, deposition,..."
Tags: Replaced Visual edit
Biljana (talk | contribs)
Line 9: Line 9:
==== Standard nitride deposition ====
==== Standard nitride deposition ====


=== STD LS Nitride2 at 300C ===
=== STD LS Nitride2 ===


==== Standard low stress nitride deposition ====
==== Standard low stress nitride deposition ====

Revision as of 23:43, 22 April 2020

There are three standard recipes : STD SiO2, STD Nitride2, and STD LS Nitride2 at 300C. Instructions bellow explain how to run each of the recipes ( seasoning, deposition, cleaning)

STD SiO2

Standard oxide deposition

STD Nitride2

Standard nitride deposition

STD LS Nitride2

Standard low stress nitride deposition