Difference between revisions of "Dry Etching Recipes"
Jump to navigation
Jump to search
(corrected links to PR & ARC etching) |
|||
Line 518: | Line 518: | ||
| |
| |
||
|A |
|A |
||
− | |[https://wiki.nanotech.ucsb.edu/wiki |
+ | |[https://wiki.nanotech.ucsb.edu/wiki/RIE_Etching_Recipes#Photoresist_and_ARC_.28RIE_5.29 R] |
| |
| |
||
+ | |[https://wiki.nanotech.ucsb.edu/wiki/ICP_Etching_Recipes#Photoresist_.26_ARC_.28Fluorine_ICP_Etcher.29 R] |
||
− | | |
||
− | |[https://wiki.nanotech.ucsb.edu/wiki |
+ | |[https://wiki.nanotech.ucsb.edu/wiki/ICP_Etching_Recipes#Photoresist_and_ARC_Etching_.28Panasonic_1.29 R] |
− | |[https://wiki.nanotech.ucsb.edu/wiki |
+ | |[https://wiki.nanotech.ucsb.edu/wiki/ICP_Etching_Recipes#Photoresist_and_ARC_etching_.28Panasonic_2.29 R] |
| |
| |
||
|A |
|A |
Revision as of 10:02, 14 June 2021
- R = Recipe is available. Clicking this link will take you to the recipe.
- A = Material is available for use, but no recipes are provided.