Difference between revisions of "Automated Wafer Cleaver (Loomis LSD-155LT)"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
 
(2 intermediate revisions by 2 users not shown)
Line 1: Line 1:
 
{{tool2|{{PAGENAME}}
 
{{tool2|{{PAGENAME}}
|picture=LoomisLSD155lt.jpg
+
|picture=IMG_0554.jpg
 
|type = Packaging
 
|type = Packaging
 
|super= Aidan Hopkins
 
|super= Aidan Hopkins
Line 25: Line 25:
 
==Operating Procedures==
 
==Operating Procedures==
   
*[https://wiki.nanotech.ucsb.edu/LoomisSOP.pdf Loomis LSD-155LT Standard Operating Procedure]
+
*[https://wiki.nanofab.ucsb.edu/w/images/d/d6/Loomis_Scriber_SOP.docx Loomis LSD-155LT Standard Operating Procedure]
   
 
==Recipes==
 
==Recipes==
   
*Recipes > Packaging > '''Wafer Cleaver Recipes (LSD-155LT)'''
+
*Recipes > Packaging > '''[[Wafer Cleaver Recipes (LSD-155LT)]]'''
 
*Wafer thinning is critical, see the Wafer Lapping (Allied XYZ) tool as well.
 
*Wafer thinning is critical, see the Wafer Lapping (Allied XYZ) tool as well.

Latest revision as of 08:16, 26 September 2023

Automated Wafer Cleaver (Loomis LSD-155LT)
IMG 0554.jpg
Location Backend Lab: ESB 1111
Tool Type Packaging
Manufacturer Loomis Industries Inc.
Model LSD-155LT
Description Loomis Automated Wafer Cleaver

Primary Supervisor Aidan Hopkins
(805) 893-2343
hopkins@ece.ucsb.edu

Materials III-V's, thin Silicon
Recipes


About

The Loomis LSD-155Lt is a production scribe and break system that can be used for processing large grids, arrays of laser bars, cleaving high quality mirror facets, and dicing wafers.

Detailed Specifications

  • Maximum Wafer Size: 4"
  • Parts mounted to low tack tape and used in conjunction with 6" plastic rings.
  • Automated cut maps at multiple angles (0° and 90° typical)
  • ~few micron alignment to on-wafer features.
  • Multiple scribe and cleave options including 'scribe and break', 'notch and cleave', and 'peck and cleave'.
  • Users should try and follow the 3 to 1 ratio (distance between cleaves should be 3X the thickness of the substrate) although some material like InP and GaAs can occasionally be cleaved closer to 2 to 1.