Surface Analysis (KLA/Tencor Surfscan): Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
Biljana (talk | contribs)
Biljana (talk | contribs)
Line 26: Line 26:
*[https://wiki.nanofab.ucsb.edu/w/images/0/04/SURFSCAN_6200_8inch_wafers.pdf Surfscan 6200 8inch wafers] *
*[https://wiki.nanofab.ucsb.edu/w/images/0/04/SURFSCAN_6200_8inch_wafers.pdf Surfscan 6200 8inch wafers] *
*[https://wiki.nanofab.ucsb.edu/w/images/d/d6/SURFSCAN_6200_6inch_wafers.pdf Surfscan 6200 6inch wafers] *
*[https://wiki.nanofab.ucsb.edu/w/images/d/d6/SURFSCAN_6200_6inch_wafers.pdf Surfscan 6200 6inch wafers] *

*[https://wiki.nanofab.ucsb.edu/w/images/8/87/SURFSCAN_6200_4inch_wafers.pdf Surfscan 6200 4inch wafers] *


*[https://wiki.nanofab.ucsb.edu/w/images/9/9f/SURFSCAN_6200_122123_for_4inch_wafers.pdf Surfscan 6200 4inch wafers] *
*[https://wiki.nanofab.ucsb.edu/w/images/9/9f/SURFSCAN_6200_122123_for_4inch_wafers.pdf Surfscan 6200 4inch wafers] *






*[https://wiki.nanofab.ucsb.edu/w/images/a/a7/SURFSCAN_6200_122123_small_substrates.pdf Surfscan 6200 [Small samples, and 2inch and 3inch wafers]] *
*[https://wiki.nanofab.ucsb.edu/w/images/a/a7/SURFSCAN_6200_122123_small_substrates.pdf Surfscan 6200 [Small samples, and 2inch and 3inch wafers]] *



Revision as of 00:45, 5 January 2024

Surface Analysis (KLA/Tencor Surfscan)
Location Bay 5
Tool Type Inspection, Test and Characterization
Manufacturer Tencor
Description Surface Analysis
KLA/Tencor Surfscan

Primary Supervisor Biljana Stamenic
(805) 893-4002
biljana@ece.ucsb.edu

Secondary Supervisor

Don Freeborn


Recipes


About

This system uses a laser-based scattering method to count size and distribution of particles (or other scattering defects) on a flat wafer surface.

It can scan wafers in size from 4 to 8 inches. Piece-parts are more difficult but can be scanned with a custom recipe.

4-inch wafers are the most standard size to measure.

For measuring very low particle counts accurately, purchase "low particle count" (LPC) wafers from a Silicon wafer vendor, and keep the wafers in the case and clean at all times until use.

Documentation

Operating Procedures



Other Documentation

  • Operations Manual
    • For detailed measurement info, it is highly recommended that you read the manual.

Examples

A low-particle 4-inch wafer example:
Gain 4: Small Particles

(0.160µm – 1.60µm)

Gain 2: Large Particles

(1.60µm – 28.0µm)

A high-particle 4-inch wafer example:
Gain 4: Small Particles

(0.160µm – 1.60µm)

Gain 2: Large Particles

(1.60µm – 28.0µm)