Thermal Evap 2 (Solder): Difference between revisions
Jump to navigation
Jump to search
(→Plot) |
|||
(5 intermediate revisions by the same user not shown) | |||
Line 23: | Line 23: | ||
*[//wiki.nanotech.ucsb.edu/w/images/b/b3/Thermal_Evaporator2.pdf Operating Instructions] |
*[//wiki.nanotech.ucsb.edu/w/images/b/b3/Thermal_Evaporator2.pdf Operating Instructions] |
||
*[https://wiki.nanofab.ucsb.edu/w/images/1/17/Thermal_Evaporator2-Normal_Fixture-_Indium_Deposition.pdf Using Normal Fixture] |
*[https://wiki.nanofab.ucsb.edu/w/images/1/17/Thermal_Evaporator2-Normal_Fixture-_Indium_Deposition.pdf Using Normal Fixture] |
||
*[https://wiki.nanofab.ucsb.edu/w/images/d/d1/Thermal_Evaprator2-Cold_Fixture-Indium_Deposition.pdf Using Cold Fixture] |
|||
== Recipes == |
== Recipes == |
||
* [[Thermal Evaporation Recipes#Thermal Evaporator 2|Recipes > Thermal Evaporation Recipes > Thermal Evaporator 2]] |
* [[Thermal Evaporation Recipes#Thermal Evaporator 2|Recipes > Thermal Evaporation Recipes > Thermal Evaporator 2]] |
||
** ''Visit this page for the materials table and evaporation parameters for all materials available.'' |
** ''Visit this page for the materials table and evaporation parameters for all materials available.'' |
||
Plot |
== Plot == |
||
* [https://wiki.nanofab.ucsb.edu/w/images/b/bb/Thermal_Evaporator2-Plot.png Plot for Indium Deposition] |
|||
* [https://docs.google.com/spreadsheets/d/1jbnKn0VP8frUMdv1K0ELFlXWh4EVV_ES0EsH2bTeTzk/edit?gid=1921661747#gid=1921661747|Plot Set vs. Desired Thickness] |
Latest revision as of 17:12, 13 March 2025
|
About
Thermal evaporator #2 is the designated "Solder" evaporator. The tool is used primarily for solder materials including Gold, Indium and Tin. See the Recipes section below for other materials used.
Use this tool for materials with low melting temperatures, or for materials that have a high risk of contamination in the e-beam evaporators.
Detailed Specifications
Wafers up to 12" can be mounted.
Documentation
Recipes
- Recipes > Thermal Evaporation Recipes > Thermal Evaporator 2
- Visit this page for the materials table and evaporation parameters for all materials available.