Thermal Evaporation Recipes: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
Biljana (talk | contribs)
→Materials Table: Updating info for Sn deposition in Thermal evaporator
Biljana (talk | contribs)
 
(One intermediate revision by the same user not shown)
Line 356: Line 356:
|0.841
|0.841
|120
|120
|Used often
|Used often, tooling factor needs adjustment
|-
|-
|Indium antimonide
|Indium antimonide
Line 572: Line 572:
|7.30
|7.30
|0.724
|0.724
|200
|197
|Program #9, Tooling factor=200%, cold fixture
|Program #9, Tooling factor=200%, cold fixture
|-
|-

Latest revision as of 21:27, 19 June 2025

Back to Vacuum Deposition Recipes.

Thermal Evaporator 1

Materials Table

Thermal Evaporator 2

Materials Table

In Deposition (Thermal Evaporator 2)