High Temp Oven (Blue M): Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
tool id included for SUM link
add toolactions
 
(3 intermediate revisions by 2 users not shown)
Line 1: Line 1:
{{tool|{{PAGENAME}}
{{tool2|{{PAGENAME}}
|picture=BlueMOven.jpg
|picture=BlueMOven.jpg
|type = Lithography
|type = Lithography
|super= Mike Silva
|super= Michael Barreraz
|super2= Aidan Hopkins
|location=Bay 5
|location=Bay 5
|description = High Temperature Oven
|description = High Temperature Oven
|manufacturer = Blue M Electric
|manufacturer = Blue M Electric
|toolid=56
|toolid=56
}}
⚫
}}The Blue M oven has a Nitrogen purge (manual flow) and is able to be programmed for a series of custom temperature ramps and holds, with a maximum temperature of 350°C. It is not actively cooled.
{{ToolActions
|toolid = 56
|ProcessControlURL =
|ProceduresURL =
|TrainingURL =
}}
⚫
The Blue M oven has a Nitrogen purge (manual flow) and is able to be programmed for a series of custom temperature ramps and holds, with a maximum temperature of 350°C. It is not actively cooled.


Numerous spin-on dielectrics and polymers are often cured in this oven, such as BCB, SU-8 and Polyimide.
Numerous spin-on dielectrics and polymers are often cured in this oven, such as BCB, SU-8 and Polyimide.

<br />

== Operating Procedures ==


[https://wiki.nanotech.ucsb.edu/w/images/6/6c/BlueM_Instructions.pdf BlueM Oven Instructions]

Latest revision as of 08:14, 6 December 2025

High Temp Oven (Blue M)
Location Bay 5
Tool Type Lithography
Manufacturer Blue M Electric
Description High Temperature Oven

Primary Supervisor Michael Barreraz
(805) 893-4147
mikebarreraz@ece.ucsb.edu

Secondary Supervisor

Aidan Hopkins


Recipes

SignupMonkey: Sign up for this tool


Instructions + Procedures

Sign Up

Get Trained

Maintenance
Messages
Report Issue


The Blue M oven has a Nitrogen purge (manual flow) and is able to be programmed for a series of custom temperature ramps and holds, with a maximum temperature of 350°C. It is not actively cooled.

Numerous spin-on dielectrics and polymers are often cured in this oven, such as BCB, SU-8 and Polyimide.


Operating Procedures

BlueM Oven Instructions