Difference between revisions of "Thermal Evap 2 (Solder)"
Jump to navigation
Jump to search
Line 50: | Line 50: | ||
|1.85 |
|1.85 |
||
|0.543 |
|0.543 |
||
+ | | |
||
+ | | |
||
+ | |- |
||
+ | |Boron |
||
+ | |B |
||
+ | |2.54 |
||
+ | |0.389 |
||
+ | | |
||
+ | | |
||
+ | |- |
||
+ | |Cadmium |
||
+ | |Cd |
||
+ | |8.64 |
||
+ | |0.682 |
||
+ | | |
||
+ | | |
||
+ | |- |
||
+ | |Cadmium sulfide |
||
+ | |CdS |
||
+ | |4.83 |
||
+ | |1.02 |
||
+ | | |
||
+ | | |
||
+ | |- |
||
+ | |Cadmium telluride |
||
+ | |CdTe |
||
+ | |5.85 |
||
+ | |0.980 |
||
| |
| |
||
| |
| |
Revision as of 16:20, 28 August 2012
|
About
Materials Table
Materials Table
| |||||
---|---|---|---|---|---|
Material | Symbol | Density, g/cm3 | Z Ratio | Tooling, % | Comments |
Aluminum | Al | 2.70 | 1.08 | ||
Antimony | Sb | 2.70 | 0.768 | ||
Arsenic | As | 5.73 | 0.996 | ||
Beryllium | Be | 1.85 | 0.543 | ||
Boron | B | 2.54 | 0.389 | ||
Cadmium | Cd | 8.64 | 0.682 | ||
Cadmium sulfide | CdS | 4.83 | 1.02 | ||
Cadmium telluride | CdTe | 5.85 | 0.980 |