Sputtering Recipes: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
No edit summary |
No edit summary |
||
| Line 5: | Line 5: | ||
=[[Sputter 4 (AJA ATC 2200-V)]]= |
=[[Sputter 4 (AJA ATC 2200-V)]]= |
||
=[[Sputter 5 (Lesker AXXIS)]]= |
=[[Sputter 5 (Lesker AXXIS)]]= |
||
=[[Ion Beam Deposition (Veeco NEXUS)]]= |
|||
==SiO{{sub|2}} deposition (IBD)== |
|||
*{{fl|IBD-SiO2-Recipe.pdf|SiO{{Sub|2}} dep}} |
|||
==SiN deposition (IBD)== |
|||
*{{fl|SiNfilm.pdf|SiN Film Data (IBD)}} |
|||
*{{fl|SiNrecipedetails.pdf|SiN Recipe Details (IBD)}} |
|||
==Ta{{sub|2}}O{{sub|5}} deposition (IBD)== |
|||
*{{fl|IBD-Ta2O5-Recipe.pdf|Ta{{sub|2}}O{{sub|5}} dep}} |
|||
Revision as of 15:35, 7 September 2012
Back to Vacuum Deposition Recipes.