=[[Thermal Evaporator 1]]=
=[[Thermal Evaporator 1]]=


=Materials Table=
==Materials Table==


{| border="1" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center; font-size: 95%" class="collapsible collapsed wikitable"
{| border="1" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center; font-size: 95%" class="collapsible collapsed wikitable"
Line 215: Line 215:
|0.1
|0.1
|
|
|-
|}


=[[Thermal Evaporator 2]]=
=[[Thermal Evaporator 2]]=


⚫
== Materials Table ==
⚫
== In Deposition (Thermal Evaporator 2) ==
⚫
*[[media:Thermal evaporator 2 Sheet1.pdf|Indium evaporation Data]]

⚫
= Materials Table =


{| border="1" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center; font-size: 95%" class="collapsible collapsed wikitable"
{| border="1" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center; font-size: 95%" class="collapsible collapsed wikitable"
Line 359: Line 356:
|0.841
|0.841
|120
|120
|Used often
|Used often, tooling factor needs adjustment
|-
|-
|Indium antimonide
|Indium antimonide
Line 575: Line 572:
|7.30
|7.30
|0.724
|0.724
|
|197
|Program #9, Tooling factor=200%, cold fixture
|Used often
|-
|-
|Titanium
|Titanium
Line 647: Line 644:
|
|
|
|
|-
|}

⚫
== In Deposition (Thermal Evaporator 2) ==
⚫
*[[Media:Thermal evaporator 2-new Sheet1.pdf|Indium evaporation Data]]