GCA 6300 Reboot Procedures: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
Biljana (talk | contribs)
No edit summary
Biljana (talk | contribs)
reboot and shutdwon-start up
 
(One intermediate revision by the same user not shown)
Line 1: Line 1:
Reboot – When terminal keyboard locks up (frozen keyboard), etc.
'''Reboot – When terminal keyboard locks up (frozen keyboard), etc.'''


1. If the terminal keyboard (the main keyboard used for alignment) is not responding, first make sure the NO SCRL key was not pressed (on the main keyboard). This gives the appearance that the keyboard is locked up, but the screen has just been paused.
1.If the terminal keyboard (the main keyboard used for alignment) is not responding, first make sure the NO SCRL key was not pressed (on the main keyboard). This gives the appearance that the keyboard is locked up, but the screen has just been paused.

2. On the terminal keyboard (the main keyboard), press together Ctrl and ]
2.On the terminal keyboard (the main keyboard), press together Ctrl and ]
] this is right bracket on the keyboard
* ] this is right bracket on the keyboard
This exits the terminal and returns control to the MOP PC(#1).
* This exits the terminal and returns control to the MOP PC(#1).
⚫
3. Pull out the PC keyboard (the upper keyboard, it is located right above the main keyboard) and press Scroll Lock twice. This toggles the KVM switch from the Smart Set PC (#2) to the MOP PC (#1).

⚫
4. Using the mouse, select ALT + X to exit (bottom off the screen). You can also type ALT + X on the upper keyboard. A window will open asking to power down the Stepper, click OK. The PC will exit to DOS.
⚫
3.Pull out the PC keyboard (the upper keyboard, it is located right above the main keyboard) and press Scroll Lock twice. This toggles the KVM switch from the Smart Set PC (#2) to the MOP PC (#1).
⚫
5. At this point you can either restart the software from DOS or turn the MOP PC (#1) off and on. To restart from DOS, enter stepper at the DOS prompt.

⚫
6. The main menu for the MOP PC (#1) should appear on the top monitor once the software/PC boots up. Pullout the PC keyboard (upper keyboard) and using the mouse, select Operate Stepper -> Start. Put the keyboard away ( push in on the sides to slide the keyboard in) .
⚫
4.Using the mouse, select ALT + X to exit (bottom off the screen). You can also type ALT + X on the upper keyboard. A window will open asking to power down the Stepper, click OK. The PC will exit to DOS.
⚫
7. The terminal will ask you to enter the time. Enter the time and date as in this example: 14:25 24-APR-19 and press Enter (the return key)

⚫
8. LOG IN [10,1], type ORIG . The stage will find its origin and then go back to the load position
⚫
5.At this point you can either restart the software from DOS or turn the MOP PC (#1) off and on. To restart from DOS, enter stepper at the DOS prompt.
⚫
9. Log out

⚫
6.The main menu for the MOP PC (#1) should appear on the top monitor once the software/PC boots up. Pullout the PC keyboard (upper keyboard) and using the mouse, select Operate Stepper -> Start. Put the keyboard away ( push in on the sides to slide the keyboard in) .

⚫
7.The terminal will ask you to enter the time. Enter the time and date as in this example: 14:25 24-APR-19 and press Enter (the return key)

⚫
8.LOG IN [10,1], type ORIG . The stage will find its origin and then go back to the load position

⚫
9.Log out

'''GCA 6300 Shutdown and''' '''Start-up''' '''(Staff only)'''

Shutdown – Should be performed when doing a lamp change

1.     Turn off lamp power supply.

2.     Turn off the DSW/AWH Control.

3.     Turn off the Stage Control.

4.     On the terminal keyboard, type Ctrl + ]                                    

This exits the terminal and returns control to the MOP PC.

5.     Turn off the terminal. The power switch is located on the top, near the front right side. You can pull out the terminal a little if needed, just be careful with the cable above the terminal.

6.     Pullout the PC keyboard and press Scroll Lock twice. This toggles the KVM switch from the Smart Set PC (#2) to the MOP PC (#1).

7.     Using the mouse, select ALT + X to exit (bottom off the screen). You can also type ALT + X on the keyboard. A window will open asking to power down the Stepper, click OK. The PC will exit to DOS.

8.     Turn off the Smart Set PC (#2).

9.     Turn off the MOP PC (#1).

10.  Turn off the Interface Chassis.

Start-up

1.     Turn on the lamp power supply and ignite the lamp.

2.     Turn on the DSW/AWH Control.

3.     Turn on the Stage Control.

4.     Turn on the terminal.

5.     Turn on the Smart Set PC (#2).

6.     Turn on the MOP PC (#1).

7.     Turn on the Interface Chassis.

8.     The main menu for the MOP PC should appear on the top monitor once the PC boots up. Pullout the PC keyboard and using the mouse, select Operate Stepper -> Start. Put the keyboard away.

9.     The terminal will ask you to enter the time (24hr) and Date (e.g. 30-APR-19).

10.  Log in and type OR. The stage should find its origin and then go back to the load position.

11.  Log out.

Latest revision as of 16:44, 7 May 2021

Reboot – When terminal keyboard locks up (frozen keyboard), etc.

1.If the terminal keyboard (the main keyboard used for alignment) is not responding, first make sure the NO SCRL key was not pressed (on the main keyboard). This gives the appearance that the keyboard is locked up, but the screen has just been paused.

2.On the terminal keyboard (the main keyboard), press together Ctrl and ]

  • ] this is right bracket on the keyboard
  • This exits the terminal and returns control to the MOP PC(#1).

3.Pull out the PC keyboard (the upper keyboard, it is located right above the main keyboard) and press Scroll Lock twice. This toggles the KVM switch from the Smart Set PC (#2) to the MOP PC (#1).

4.Using the mouse, select ALT + X to exit (bottom off the screen). You can also type ALT + X on the upper keyboard. A window will open asking to power down the Stepper, click OK. The PC will exit to DOS.

5.At this point you can either restart the software from DOS or turn the MOP PC (#1) off and on. To restart from DOS, enter stepper at the DOS prompt.

6.The main menu for the MOP PC (#1) should appear on the top monitor once the software/PC boots up. Pullout the PC keyboard (upper keyboard) and using the mouse, select Operate Stepper -> Start. Put the keyboard away ( push in on the sides to slide the keyboard in) .

7.The terminal will ask you to enter the time. Enter the time and date as in this example: 14:25 24-APR-19 and press Enter (the return key)

8.LOG IN [10,1], type ORIG . The stage will find its origin and then go back to the load position

9.Log out

GCA 6300 Shutdown and Start-up (Staff only)

Shutdown – Should be performed when doing a lamp change

1.     Turn off lamp power supply.

2.     Turn off the DSW/AWH Control.

3.     Turn off the Stage Control.

4.     On the terminal keyboard, type Ctrl + ]                                    

This exits the terminal and returns control to the MOP PC.

5.     Turn off the terminal. The power switch is located on the top, near the front right side. You can pull out the terminal a little if needed, just be careful with the cable above the terminal.

6.     Pullout the PC keyboard and press Scroll Lock twice. This toggles the KVM switch from the Smart Set PC (#2) to the MOP PC (#1).

7.     Using the mouse, select ALT + X to exit (bottom off the screen). You can also type ALT + X on the keyboard. A window will open asking to power down the Stepper, click OK. The PC will exit to DOS.

8.     Turn off the Smart Set PC (#2).

9.     Turn off the MOP PC (#1).

10.  Turn off the Interface Chassis.

Start-up

1.     Turn on the lamp power supply and ignite the lamp.

2.     Turn on the DSW/AWH Control.

3.     Turn on the Stage Control.

4.     Turn on the terminal.

5.     Turn on the Smart Set PC (#2).

6.     Turn on the MOP PC (#1).

7.     Turn on the Interface Chassis.

8.     The main menu for the MOP PC should appear on the top monitor once the PC boots up. Pullout the PC keyboard and using the mouse, select Operate Stepper -> Start. Put the keyboard away.

9.     The terminal will ask you to enter the time (24hr) and Date (e.g. 30-APR-19).

10.  Log in and type OR. The stage should find its origin and then go back to the load position.

11.  Log out.