AZ5214 is a positive PR to start. If you expose and develop, then the exposed areas develop out like a typical positive PR.
AZ5214 is a positive PR to start. If you expose and develop, then the exposed areas develop out like a typical positive PR.
[[File:AZ5214 Fabublox Positive PR schematic.png|none|thumb|Positive operation with NO PEB.]]
[[File:AZ5214 Fabublox Positive PR schematic.png|none|thumb|Positive operation with NO PEB nor Flood Expose. [''Schematic produced via [http://fabublox.com Fabublox]''<nowiki>]</nowiki>|399x399px]]
However if instead you expose, then post-exposure-Bake “PEB”, the exposed areas become Hardened/impervious to developer. But the rest of the PR is still unexposed.
However if instead you expose, then post-exposure-Bake “PEB”, the exposed areas become Hardened/impervious to developer. But the rest of the PR is still unexposed.


So THEN you flood expose the rest of the unexposed PR, and like a positive PR this now allows that PR to develop out.
So THEN you flood expose the rest of the unexposed PR, and like a positive PR this now allows that PR to develop out.
[[File:AZ5214 negative process schematic.png|alt=2D schematic of AZ5214 negative PR process|none|thumb|594x594px|Negative operation - requiring PEB and Flood Expose]]


=== Basic Process Flow ===

A Basic 5214 the process should look like:
A Basic 5214 the process should look like:


• Spin + soft-bake
* Spin + soft-bake
⚫
* MLA expose

⚫
* P.E.Bake - harden the exposed PR, making it "negative"
⚫
• MLA expose
⚫
* Flood expose - expose the remaining positive PR

⚫
* Develop
⚫
• P.E.Bake - harden the exposed PR, making it "negative"

⚫
• Flood expose - expose the remaining positive PR

⚫
• Develop

Latest revision as of 23:39, 22 August 2024

AZ5214 is a positive PR to start. If you expose and develop, then the exposed areas develop out like a typical positive PR.

Positive operation with NO PEB nor Flood Expose. [Schematic produced via Fabublox]

However if instead you expose, then post-exposure-Bake “PEB”, the exposed areas become Hardened/impervious to developer. But the rest of the PR is still unexposed.

So THEN you flood expose the rest of the unexposed PR, and like a positive PR this now allows that PR to develop out.

2D schematic of AZ5214 negative PR process
Negative operation - requiring PEB and Flood Expose

Basic Process Flow

A Basic 5214 the process should look like:

  • Spin + soft-bake
  • MLA expose
  • P.E.Bake - harden the exposed PR, making it "negative"
  • Flood expose - expose the remaining positive PR
  • Develop