Resistivity Mapper (CDE RESMAP): Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
Created page with "{{tool|{{PAGENAME}} |picture=CDEResmap.jpg |type = Inspection, Test and Characterization |super= Tony Bosch |phone=(805)839-3918x217 |location=Bay ? |email=bosch@ece.ucsb.edu |de…" |
Millerski w (talk | contribs) Updated SOP |
||
| (6 intermediate revisions by 4 users not shown) | |||
| Line 1: | Line 1: | ||
{{ |
{{tool2|{{PAGENAME}} |
||
|picture=CDEResmap.jpg |
|picture=CDEResmap.jpg |
||
|type = Inspection, Test and Characterization |
|type = Inspection, Test and Characterization |
||
|super= |
|super= Bill Millerski |
||
|super2= Tony Bosch |
|||
|phone=(805)839-3918x217 |
|phone=(805)839-3918x217 |
||
|location=Bay ? |
|location=Bay ? |
||
| Line 10: | Line 11: | ||
|materials = |
|materials = |
||
}} |
}} |
||
= |
=About= |
||
The CDE Resmap 4 point resistivity mapper is used for measuring resistivity across the wafer for substrates and thin films deposited in the facility. The system can do automated resistivity mapping for pieces to 8 inch wafers. |
The CDE Resmap 4 point resistivity mapper is used for measuring resistivity across the wafer for substrates and thin films deposited in the facility. The system can do automated resistivity mapping for pieces to 8 inch wafers. |
||
The resistivity range is 2 mOhm/Square to 5 MOhm/square. Contour plots, 3D plots, histograms, data exporting are supported from the Windows XP based control system. |
|||
==Instructions== |
|||
*[[CDE ResMap Quick-Start instructions]] |
|||
*[https://wiki.nanofab.ucsb.edu/w/images/3/37/CDE_ResMap_Operating_Instructions.pdf CDE ResMap Operating Instructions] |
|||
*System can export CSV files - contact supervisor for instructions. |
|||
Latest revision as of 22:07, 30 October 2023
| ||||||||||||||||||||||||||
About
The CDE Resmap 4 point resistivity mapper is used for measuring resistivity across the wafer for substrates and thin films deposited in the facility. The system can do automated resistivity mapping for pieces to 8 inch wafers.
The resistivity range is 2 mOhm/Square to 5 MOhm/square. Contour plots, 3D plots, histograms, data exporting are supported from the Windows XP based control system.
Instructions
- CDE ResMap Quick-Start instructions
- CDE ResMap Operating Instructions
- System can export CSV files - contact supervisor for instructions.