PECVD1 Recipes: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
| Line 12: | Line 12: | ||
== Other recipes (PECVD1)== |
== Other recipes (PECVD1)== |
||
| ⚫ | |||
*[[media:PECVD1-LS SION recipe 2014.pdf|SiO<sub>x</sub>N<sub>y</sub> Recipe]] |
*[[media:PECVD1-LS SION recipe 2014.pdf|SiO<sub>x</sub>N<sub>y</sub> Recipe]] |
||
*[https://docs.google.com/spreadsheets/d/1rixyzAAq6q08M5OwvZiDVoh3K8B566XKM-UZAQIAnsg/edit#gid=sharing SiO<sub>x</sub>N<sub>y</sub> Data December 2014] |
*[https://docs.google.com/spreadsheets/d/1rixyzAAq6q08M5OwvZiDVoh3K8B566XKM-UZAQIAnsg/edit#gid=sharing SiO<sub>x</sub>N<sub>y</sub> Data December 2014] |
||
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dEttR2JSTkRoamR0SUZ4bE5QUW9uS2c&usp=sharing SiO<sub>x</sub>N<sub>y</sub> 3000A Thickness uniformity 2014] |
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dEttR2JSTkRoamR0SUZ4bE5QUW9uS2c&usp=sharing SiO<sub>x</sub>N<sub>y</sub> 3000A Thickness uniformity 2014] |
||
| ⚫ | |||
*[https://docs.google.com/spreadsheets/d/1Joz0az9TGZWQc4CiMQJZzLBbNFbx_hH2Oc0B4NNJmYk/edit#gid=978933038=sharing LS SiN Data December 2014] |
*[https://docs.google.com/spreadsheets/d/1Joz0az9TGZWQc4CiMQJZzLBbNFbx_hH2Oc0B4NNJmYk/edit#gid=978933038=sharing LS SiN Data December 2014] |
||
*[https://docs.google.com/spreadsheets/d/1xIzc2CufRYNSfAtsOXpw3IzHreeu42BWrLBV0kzP6kA/edit#gid=481681015=sharing LS SiN 3000A Thickness uniformity 2014] |
*[https://docs.google.com/spreadsheets/d/1xIzc2CufRYNSfAtsOXpw3IzHreeu42BWrLBV0kzP6kA/edit#gid=481681015=sharing LS SiN 3000A Thickness uniformity 2014] |
||
Revision as of 16:59, 10 December 2014
PECVD 1 (PlasmaTherm 790)
SiN deposition (PECVD #1)
SiO2 deposition (PECVD #1)
Other recipes (PECVD1)
- SiOxNy Recipe
- SiOxNy Data December 2014
- SiOxNy 3000A Thickness uniformity 2014
- LS SiN Recipe
- LS SiN Data December 2014
- LS SiN 3000A Thickness uniformity 2014
LS SiOxNy deposition (PECVD #1)
- SiOxNy Deposition Recipes - Varying N/O Ratio
- SiOxNy Stress/Index vs. O/N Ratio
- SiOxNy Recipe
- SiOxNy Data December 2014
- SiOxNy 3000A Thickness uniformity 2014