== SiO<sub>2</sub> deposition (PECVD #1) ==
== SiO<sub>2</sub> deposition (PECVD #1) ==
*[[media:PECVD1-SiO2-standard recipe 2014 SiO2 standard recipe.pdf|SiO<sub>2</sub> Standard Recipe]]
*[[media:NewPECVD1-SiO2-standard recipe 2014.pdf|SiO<sub>2</sub> Standard Recipe]]
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dEw0bjFEdTF2SUhRa25Ca0d0SzBha3c&usp=drive_web#gid=sharing SiO<sub>2</sub> Data 2014]
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dEw0bjFEdTF2SUhRa25Ca0d0SzBha3c&usp=drive_web#gid=sharing SiO<sub>2</sub> Data 2014]
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dDQ3VEtZQVRpdVdlbGtIZHpTNmFzNmc&usp=drive_web#gid=sharing SiO<sub>2</sub> 1000A Thickness uniformity 2014]
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dDQ3VEtZQVRpdVdlbGtIZHpTNmFzNmc&usp=drive_web#gid=sharing SiO<sub>2</sub> 1000A Thickness uniformity 2014]