Stepper 2 (AutoStep 200): Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
No edit summary
moved PR's out of paragraph into separate table.
Line 12: Line 12:
}}
}}


= About =
== About ==


Our GCA wafer stepper is an i-line (365 nm) step and repeat exposure tool for doing lithography that requires high resolution and/or critical alignment. The system has been modified to accept piece parts (down to smaller than 10mm x 10mm) up to 6” diameter wafers using manual wafer loading. The maximum square die size is 14.8 mm x 14.8 mm. The system has an Olympus 2145 (N.A. = 0.45) lens that reduces the mask image by 5 x and gives an ultimate resolution of better than 0.5 um in the center of the lens field. The system can easily produce 0.7 um isolated lines across the entire field. The Autostep200 system has 3-point wafer leveling to improve focus uniformity across the field. Autofocus is used to determine the sample surface relative to the lens, making the focus stable and repeatable for different thickness of wafer. The stages are controlled by stepper motors and laser interferometers. Using the global, manual alignment, better than 0.25 um alignment error is achievable. Using the DFAS local alignment system, alignment error better than 0.15 um is achieved. With the 1000 W Hg arc lamp, we get about 420 mW/cm² of i-line intensity at the wafer.
Our GCA wafer stepper is an i-line (365 nm) step and repeat exposure tool for doing lithography that requires high resolution and/or critical alignment. The system has been modified to accept piece parts (down to smaller than 10mm x 10mm) up to 6” diameter wafers using manual wafer loading. The maximum square die size is 14.8 mm x 14.8 mm. The system has an Olympus 2145 (N.A. = 0.45) lens that reduces the mask image by 5 x and gives an ultimate resolution of better than 0.5 um in the center of the lens field. The system can easily produce 0.7 um isolated lines across the entire field. The Autostep200 system has 3-point wafer leveling to improve focus uniformity across the field. Autofocus is used to determine the sample surface relative to the lens, making the focus stable and repeatable for different thickness of wafer. The stages are controlled by stepper motors and laser interferometers. Using the global, manual alignment, better than 0.25 um alignment error is achievable. Using the DFAS local alignment system, alignment error better than 0.15 um is achieved. With the 1000 W Hg arc lamp, we get about 420 mW/cm² of i-line intensity at the wafer.


The system is computer controlled with the capability to program and save a wide variety of exposure jobs. We also have unlimited phone support for system problems through a service contract. The laboratory contains a variety of i-line compatible photoresists. 955CM-0.9 for 0.7-1.0 um thick positive processes. AZ5214E for 1.0 um thick image reversal (negative) process. SPR955CM-1.8 for 1.5-2.0 um thick positive processes. SPR220-3 for 2.5-5 um thick positive process. SPR220-7 for >5 um thick positive processes. AZnLOF5510 for <1.0um and AZnLOF 2020 for 1.5-3 um negative resist process. Shipley LOL-2000 is also used as an underlayer for high resolution lift-off processes.
The system is computer controlled with the capability to program and save a wide variety of exposure jobs. We also have unlimited phone support for system problems through a service contract.


=Detailed Specifications=
==Detailed Specifications==
*Lens: Olympus 2145: NA = 0.45; Depth of field = 1.2 um for 0.6 um process
*Lens: Olympus 2145: NA = 0.45; Depth of field = 1.2 um for 0.6 um process
*Maximum die size: ~ 15 mm x 15 mm
*Maximum die size: ~ 15 mm x 15 mm
Line 27: Line 27:
*Reticle alignment fiducials and global/local fiducials available
*Reticle alignment fiducials and global/local fiducials available


= Process Information =
== Process Information ==


*[http://signupmonkey.ece.ucsb.edu/wiki/index.php/Lithography_Recipes Process Page]
*[https://signupmonkey.ece.ucsb.edu/wiki/index.php/Lithography_Recipes#Photolithography_Recipes Process Page: Photolithography Recipes]


=== Photoresists: ===
=Service Provider=
*The laboratory contains a variety of i-line compatible photoresists. See the [https://signupmonkey.ece.ucsb.edu/wiki/index.php/Lithography_Recipes#Photolithography_Recipes Photolith. Recipes Page] for detailed processing info (bakes/spins/exposure does etc.). Basic photoresists include:
**955CM-0.9 for 0.7-1.0 um thick positive processes.
**AZ5214E for 1.0 um thick image reversal (negative) process.
**SPR955CM-1.8 for 1.5-2.0 um thick positive processes.
**SPR220-3 for 2.5-5 um thick positive process.
**SPR220-7 for >5 um thick positive processes.
**AZnLOF5510 for <1.0um and AZnLOF 2020 for 1.5-3 um negative resist process.
**Shipley LOL-2000 is also used as an underlayer for high resolution lift-off processes.

==Service Provider==
* [http://3ctechnical.com/index.html 3C Technical] - The company that services the stepper.
* [http://3ctechnical.com/index.html 3C Technical] - The company that services the stepper.


=Operating Procedures=
==Operating Procedures==
* [[media:Autostep 200 Training Manual-4-10-15 .pdf|Training Manual]]
* [[media:Autostep 200 Training Manual-4-10-15 .pdf|Training Manual]]

Revision as of 23:45, 7 December 2018

Stepper 2 (AutoStep 200)
Tool Type Lithography
Location Bay 6
Supervisor Biljana Stamenic
Supervisor Phone (805) 893-4002
Supervisor E-Mail biljana@ece.ucsb.edu
Description GCA 200 I-Line Wafer Stepper
Manufacturer GCA
Sign up for this tool



About

Our GCA wafer stepper is an i-line (365 nm) step and repeat exposure tool for doing lithography that requires high resolution and/or critical alignment. The system has been modified to accept piece parts (down to smaller than 10mm x 10mm) up to 6” diameter wafers using manual wafer loading. The maximum square die size is 14.8 mm x 14.8 mm. The system has an Olympus 2145 (N.A. = 0.45) lens that reduces the mask image by 5 x and gives an ultimate resolution of better than 0.5 um in the center of the lens field. The system can easily produce 0.7 um isolated lines across the entire field. The Autostep200 system has 3-point wafer leveling to improve focus uniformity across the field. Autofocus is used to determine the sample surface relative to the lens, making the focus stable and repeatable for different thickness of wafer. The stages are controlled by stepper motors and laser interferometers. Using the global, manual alignment, better than 0.25 um alignment error is achievable. Using the DFAS local alignment system, alignment error better than 0.15 um is achieved. With the 1000 W Hg arc lamp, we get about 420 mW/cm² of i-line intensity at the wafer.

The system is computer controlled with the capability to program and save a wide variety of exposure jobs. We also have unlimited phone support for system problems through a service contract.

Detailed Specifications

  • Lens: Olympus 2145: NA = 0.45; Depth of field = 1.2 um for 0.6 um process
  • Maximum die size: ~ 15 mm x 15 mm
  • Resolution: 400-450 nm for R&D; 700 nm over entire 15 mm x 15 mm field
  • Registration tolerance: 0.25um global alignment; Max 0.15 um local alignment (with care, you can achieve < 0.10 um registration)
  • Minimum substrate size: ~ 10 x 10 mm
  • Computer programmable, recipes saved on hard disk
  • Reticle alignment fiducials and global/local fiducials available

Process Information

Photoresists:

  • The laboratory contains a variety of i-line compatible photoresists. See the Photolith. Recipes Page for detailed processing info (bakes/spins/exposure does etc.). Basic photoresists include:
    • 955CM-0.9 for 0.7-1.0 um thick positive processes.
    • AZ5214E for 1.0 um thick image reversal (negative) process.
    • SPR955CM-1.8 for 1.5-2.0 um thick positive processes.
    • SPR220-3 for 2.5-5 um thick positive process.
    • SPR220-7 for >5 um thick positive processes.
    • AZnLOF5510 for <1.0um and AZnLOF 2020 for 1.5-3 um negative resist process.
    • Shipley LOL-2000 is also used as an underlayer for high resolution lift-off processes.

Service Provider

Operating Procedures