The ASML 5500 stepper is a 248nm DUV stepper for imaging dense features down to below 200nm and isolated line structures down to below 150nm. Overlay accuracy is better than 30nm. The system is configured for 4” wafers and, with staff support, mounted pieces down to 14mm in size can be exposed using a 4” wafer as a carrier. The system is designed for high throughput, so shooting multiple 4" wafers is extremely fast. Additionally, the litho programming is highly programmable, allowing for very flexible exposures of multiple aligned patterns from multiple masks in a single session, allowing for process optimization of large vs. small features in a single lithography.
The ASML 5500 stepper is a 248nm DUV stepper for imaging dense features down to below 200nm and isolated line structures down to below 150nm. Overlay accuracy is better than 30nm. The system is configured for 4” wafers and, with staff support, mounted pieces down to 14mm in size can be exposed using a 4” wafer as a carrier. The system is designed for high throughput, so shooting multiple 4" wafers is extremely fast. Additionally, the litho programming is highly programmable, allowing for very flexible exposures of multiple aligned patterns from multiple masks in a single session, allowing for process optimization of large vs. small features in a single lithography.


The full field useable exposure area is limited to the intersection of a 31mm diameter circle and a rectangle of dimensions 22mm x 27mm. The system has a variable NA system and has a square field image size of 21 x 21mm for 0.63 NA and a square field image size of 22mm x 22mm for 0.4 to 0.57 NA.
The full field useable exposure area is limited to the intersection of a 31mm diameter circle and a rectangle of dimensions 22mm x 27mm. See the [[ASML 5500 Mask Making Guidelines|Mask Making Guidelines page]] for more info on exposure field sizes and how to order your mask plates.


⚫
Resists Used (see [https://www.nanotech.ucsb.edu/wiki/index.php/Lithography_Recipes#Photolithography_Recipes PhotoLith. Recipes] for processing info):
Other rectangular sizes available: 21mm x 23mm; 20mm x 24mm; 19mm x 25mm; 18mm x 25.5mm; 17mm x 26mm; 16mm x 26.5mm; 15mm x 27mm.

⚫
Resists Used (see [https://www.nanotech.ucsb.edu/wiki/index.php/Lithography_Recipes#Photolithography_Recipes PhotoLith Recipes] for processing info):
* UV210-0.3 - Positive: 300nm nominal thickness
* UV210-0.3 - Positive: 300nm nominal thickness
* UV6-0.8 - Positive: 800nm nominal thickness
* UV6-0.8 - Positive: 800nm nominal thickness

Revision as of 22:05, 21 February 2018

Stepper 3 (ASML DUV)
Tool Type Lithography
Location Bay 3
Supervisor Brian Thibeault
Supervisor Phone (805) 893-2268
Supervisor E-Mail thibeault@ece.ucsb.edu
Description ASML PAS 5500/300 DUV Stepper
Manufacturer ASML
Sign up for this tool



About

The ASML 5500 stepper is a 248nm DUV stepper for imaging dense features down to below 200nm and isolated line structures down to below 150nm. Overlay accuracy is better than 30nm. The system is configured for 4” wafers and, with staff support, mounted pieces down to 14mm in size can be exposed using a 4” wafer as a carrier. The system is designed for high throughput, so shooting multiple 4" wafers is extremely fast. Additionally, the litho programming is highly programmable, allowing for very flexible exposures of multiple aligned patterns from multiple masks in a single session, allowing for process optimization of large vs. small features in a single lithography.

The full field useable exposure area is limited to the intersection of a 31mm diameter circle and a rectangle of dimensions 22mm x 27mm. See the Mask Making Guidelines page for more info on exposure field sizes and how to order your mask plates.

Resists Used (see PhotoLith. Recipes for processing info):

  • UV210-0.3 - Positive: 300nm nominal thickness
  • UV6-0.8 - Positive: 800nm nominal thickness
  • UV26-2.5 - Positive: 2.5um nominal thickness
  • UVN2300-0.5 - Negative: 500nm nominal thickness
  • AR2/DUV42P-6/DS-K101: Anti-Reflective Coatings
  • PMGI: Underlayer

AZ300MIF Developer for all processes

Process Information