Test Data of etching SiO2 with CHF3/CF4/O2 (using this recipe only for Fluorine etch of the underneath layer): Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
moved SEM images to table, changed "File:" link --> Direct link to file |
add one SEM pic |
||
| Line 15: | Line 15: | ||
|0.74 |
|0.74 |
||
|77.9 |
|77.9 |
||
|[https://www.nanotech.ucsb.edu/wiki/index.php/File:SiO2_Etch_using_ICP2_with_O2.pdf] |
|||
| |
|||
|- |
|- |
||
|1/28/2019 |
|1/28/2019 |
||