The lab currently has 3 Nikon Microscopes (Microscopes #2, #3 & #4). These are located in bays 6 and 7. |
The lab currently has 3 Nikon Microscopes (Microscopes #2, #3 & #4). These are located in bays 6 and 7. |
||
The scopes are connected to computers via Jenoptik ProgRes software which allows users to digitally capture images through the microscope and make calibrated measurements. |
The scopes have 3rd party cameras that are connected to computers via Jenoptik ProgRes software which allows users to digitally capture images through the microscope and make calibrated measurements. |
||
=== Microscope #2: (Bay 7) === |
=== Microscope #2: Nikon Optiphot 200 (Bay 7) === |
||
* Trinocular: Ocular Binoc. + Camera (Simultaneous) |
* Trinocular: Ocular Binoc. + Camera (Simultaneous) |
||
* ProgRes video/photo capture & user-editable calibrated measurement |
* ProgRes video/photo capture & user-editable calibrated measurement |
||
| Line 20: | Line 20: | ||
* Differential Interference Contrast (DIC/Nomarski) |
* Differential Interference Contrast (DIC/Nomarski) |
||
** ''The DIC prism is installed on each objective and can't be removed, so even regular microscope images suffer from a slight double-image'' |
** ''The DIC prism is installed on each objective and can't be removed, so even regular microscope images suffer from a slight double-image'' |
||
* Top Illumination |
* Top Reflected Illumination (Episcopic) |
||
=== Microscope #3: |
=== Microscope #3: Nikon Eclipse L200 (Bay 6) === |
||
* [https://www.nanotech.ucsb.edu/wiki/images/8/80/Nikon-Microscope-Manual.pdf Manual for Nikon Eclipse L200D] |
* [https://www.nanotech.ucsb.edu/wiki/images/8/80/Nikon-Microscope-Manual.pdf Manual for Nikon Eclipse L200D] |
||
* Trinocular: Binoc. + Camera (Mutually Exclusive) |
* Trinocular: Binoc. + Camera (Mutually Exclusive) |
||
| Line 30: | Line 30: | ||
* Bright/Dark Field |
* Bright/Dark Field |
||
* Differential Interference Contrast (DIC/Nomarski) |
* Differential Interference Contrast (DIC/Nomarski) |
||
* Top Illumination |
* Top Reflected Illumination (Episcopic) |
||
=== Microscope #4: (Bay 6) === |
=== Microscope #4: Nikon Eclipse L200D (Bay 6) === |
||
* Trinocular: Binoc. + Camera (Mutually Exclusive) |
* Trinocular: Binoc. + Camera (Mutually Exclusive) |
||
* ProgRes video/photo capture & user-editable calibrated measurement |
* ProgRes video/photo capture & user-editable calibrated measurement |
||
| Line 39: | Line 39: | ||
* Bright/Dark Field |
* Bright/Dark Field |
||
* Differential Interference Contrast (DIC/Nomarski) |
* Differential Interference Contrast (DIC/Nomarski) |
||
* Top |
* Top Reflected (Episcopic) & Bottom Transmission (Diascopic) Illumination |
||
==Olympus== |
==Olympus== |
||
| Line 56: | Line 56: | ||
* Bright/Dark Field |
* Bright/Dark Field |
||
* Differential Interference Contrast (DIC/Nomarski) |
* Differential Interference Contrast (DIC/Nomarski) |
||
* Top |
* Top (Episcopic) & Bottom (Diascopic) Illumination |
||
* Three Fluorescence Filters (requires training, see main tool page for specs.) |
* Three Fluorescence Filters (requires training, see main tool page for specs.) |
||
Revision as of 05:55, 15 May 2019
|
Nikon
The lab currently has 3 Nikon Microscopes (Microscopes #2, #3 & #4). These are located in bays 6 and 7.
The scopes have 3rd party cameras that are connected to computers via Jenoptik ProgRes software which allows users to digitally capture images through the microscope and make calibrated measurements.
Microscope #2: Nikon Optiphot 200 (Bay 7)
- Trinocular: Ocular Binoc. + Camera (Simultaneous)
- ProgRes video/photo capture & user-editable calibrated measurement
- Objectives: 5x, 10x, 20x, 50x, 100x, 150x
- Filters: Green, ND
- Bright/Dark Field
- Differential Interference Contrast (DIC/Nomarski)
- The DIC prism is installed on each objective and can't be removed, so even regular microscope images suffer from a slight double-image
- Top Reflected Illumination (Episcopic)
Microscope #3: Nikon Eclipse L200 (Bay 6)
- Manual for Nikon Eclipse L200D
- Trinocular: Binoc. + Camera (Mutually Exclusive)
- ProgRes video/photo capture & user-editable calibrated measurement
- Objectives: 5x, 10x, 20x, 50x, 100x, 150x
- Filters: Green, ND
- Bright/Dark Field
- Differential Interference Contrast (DIC/Nomarski)
- Top Reflected Illumination (Episcopic)
Microscope #4: Nikon Eclipse L200D (Bay 6)
- Trinocular: Binoc. + Camera (Mutually Exclusive)
- ProgRes video/photo capture & user-editable calibrated measurement
- Objectives: 5x, 10x, 20x, 50x, 100x, 150x
- Filters: Green, ND
- Bright/Dark Field
- Differential Interference Contrast (DIC/Nomarski)
- Top Reflected (Episcopic) & Bottom Transmission (Diascopic) Illumination
Olympus
Microscope #1: Olympus Optiphot-2 (Bay 3)
- To be added
Fluorescence Microscope: Olympus MX51 (Bay 6)
- See the wiki page for the Olympus MX51 for full details
- Trinocular: Binoc. + Camera (Simultaneous)
- Native Olympus Stream Software:
- Photo/video capture
- Calibrated measurement (calibrations locked)
- Objectives: 5x, 10x, 20x, 50x, 100x, 150x
- Filters: Green, ND
- Bright/Dark Field
- Differential Interference Contrast (DIC/Nomarski)
- Top (Episcopic) & Bottom (Diascopic) Illumination
- Three Fluorescence Filters (requires training, see main tool page for specs.)
DUV Microscope: Olympus MX61A-DUV (Bay 7)
Please see the main Tool page for detailed info on this microscope.
YOU ARE REQUIRED TO GET TRAINED on this tool before you are allowed to use it! Please contact the Tool Owner to get training.
- Motorized Stage + Turret
- Trinocular: Binoc. + Camera (Simultaneous)
- Objectives: 5x, 10x, 20, 50x, 100x, DUV-100x
- Filters: to be added
- Native Olympus Software control with Calibrated measurements
- Deep-UV Light source + DUV Camera for DUV-100x sub-micron imaging/measurement
Olympus LEXT Confocal Microscope
See the main tool page for complete info: Laser Scanning Confocal M-scope (Olympus LEXT)
YOU ARE REQUIRED TO GET TRAINED on this tool before you are allowed to use it! Please contact the Tool Owner to get training.
- Motorized stage + Objective Turret
- 100mm wafer stage
- Native Olympus OLS2000 Software:
- Calibrated measurement (calibrations locked)
- Image stitching capabilities
- 3D Topographical measurement capabilities via laser-scanning confocal microscopy function
- Surface roughness estimations (large roughness)
- Thin-Film Film-Thickness Measurements (thicker films)