PECVD 2 (Advanced Vacuum): Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
Biljana (talk | contribs)
No edit summary
Biljana (talk | contribs)
Line 36: Line 36:
*
*
*
*
* [[Advanced Vacuum PECVD.pdf|Operating Instructions]]
* [[:File:Advanced Vacuum PECVD.pdf|Operating Instructions]]
* [[Wafer Coating Process Traveler]]
* [[Wafer Coating Process Traveler]]
* For particle counting method, see the [[Wafer scanning process traveler|Surfscan Scanning Procedure]]
* For particle counting method, see the [[Wafer scanning process traveler|Surfscan Scanning Procedure]]

Revision as of 16:58, 27 May 2020

PECVD 2 (Advanced Vacuum)
Tool Type Vacuum Deposition
Location Bay 2
Supervisor Brian Lingg
Supervisor Phone (805) 893-8145
Supervisor E-Mail lingg_b@ucsb.edu
Description Vision 310 Advanced Vacuum PECVD
Manufacturer Veeco
Vacuum Deposition Recipes
Sign up for this tool


About

This open-load system is dedicated to PECVD of SiO2, SiNx, SiOxNy, and a-Si using Silane (2%SiH4, 98% He), N2O, NH3, and N2 gases. The sample electrode has a 270mm diameter useable area, allowing for multiple 4” wafer depositions in a single run. Standard operating temperature is 300C, but can be user changed for temps ranging anywhere from 250 to 350C. The system is equipped with a dual generator, dual frequency option for growth of low-stress Nitride films.

Recipes

See Also

Documentation