Holographic Lith/PL Setup (Custom): Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
link to PL system page
→Detailed Specifications: added max sample size
Line 10: Line 10:
|toolid=35
|toolid=35
}}
}}
= About =
=About=
The interference lithography system (aka. Holography) at UCSB uses a 15mW, single-mode, 325 nm HeCd laser that is filtered and expanded by pinhole filters to produce the large area exposure beam. The system uses a simple mirror configuration with a fixed 90 degree angle between the mirror and sample. The entire mirror/sample assembly is rotated in 0.1 degree increments to change the grating pitch from ~ 200 nm to ~ 280 nm (35 to 55 degrees) over an ~ 2 cm x 2 cm exposure area.
The interference lithography system (aka. Holography) at UCSB uses a 15mW, single-mode, 325 nm HeCd laser that is filtered and expanded by pinhole filters to produce the large area exposure beam. The system uses a simple mirror configuration with a fixed 90 degree angle between the mirror and sample. The entire mirror/sample assembly is rotated in 0.1 degree increments to change the grating pitch from ~ 200 nm to ~ 280 nm (35 to 55 degrees) over an ~ 2 cm x 2 cm exposure area.


Line 16: Line 16:


A photoluminescence measurement setup is co-located on the optical table. Please see the page for the PL system for more info:
A photoluminescence measurement setup is co-located on the optical table. Please see the page for the PL system for more info:

* [[Photoluminescence PL Setup (Custom)]]
*[[Photoluminescence PL Setup (Custom)]]


=Detailed Specifications=
=Detailed Specifications=

*15 mW single TEM mode HeCd laser
*15 mW single TEM mode HeCd laser
*Max sample size: ~1.5 inch square
*~ 2 cm x 2 cm uniform exposure area
*~ 2 cm x 2 cm uniform exposure area
*~ several minute exposure times
*~ several minute exposure times

Revision as of 15:36, 22 December 2022

Holographic Lith/PL Setup (Custom)
Tool Type Lithography
Location Bay 6
Supervisor Ning Cao
Supervisor Phone (805) 893-4689
Supervisor E-Mail ningcao@ece.ucsb.edu
Description Custom Built Interference Lithography
Manufacturer Kimmon
Sign up for this tool


About

The interference lithography system (aka. Holography) at UCSB uses a 15mW, single-mode, 325 nm HeCd laser that is filtered and expanded by pinhole filters to produce the large area exposure beam. The system uses a simple mirror configuration with a fixed 90 degree angle between the mirror and sample. The entire mirror/sample assembly is rotated in 0.1 degree increments to change the grating pitch from ~ 200 nm to ~ 280 nm (35 to 55 degrees) over an ~ 2 cm x 2 cm exposure area.

THMR-3600HP resist spin-coated to ~ 80 nm thickness is used for grating exposure. 2-D gratings can be formed by rotating the sample and doing multiple exposures. Total exposure times are controlled by a manual shutter and are generally several minutes in length.

A photoluminescence measurement setup is co-located on the optical table. Please see the page for the PL system for more info:

Detailed Specifications

  • 15 mW single TEM mode HeCd laser
  • Max sample size: ~1.5 inch square
  • ~ 2 cm x 2 cm uniform exposure area
  • ~ several minute exposure times
  • Grating period adjustable from ~200 to ~280 nm with a single stage