Dry Etching Recipes: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
FL-ICP: SiN = A |
link to Oxford InP/PnGaAsP recipes |
||
| Line 323: | Line 323: | ||
|{{rl|ICP Etching Recipes|AlGaAs Etch (Panasonic 1)}} |
|{{rl|ICP Etching Recipes|AlGaAs Etch (Panasonic 1)}} |
||
| |
| |
||
| |
|A |
||
|{{rl|ICP Etching Recipes|ICP-Etch (Unaxis VLR)|GaAs-AlGaAs Etch (Unaxis VLR)|AlGaAs Etch (Unaxis VLR)}} |
|{{rl|ICP Etching Recipes|ICP-Etch (Unaxis VLR)|GaAs-AlGaAs Etch (Unaxis VLR)|AlGaAs Etch (Unaxis VLR)}} |
||
| |
| |
||
| Line 342: | Line 342: | ||
| |
| |
||
| |
| |
||
| |
|A |
||
|{{rl|ICP Etching Recipes|GaN Etch (Unaxis VLR)}} |
|{{rl|ICP Etching Recipes|GaN Etch (Unaxis VLR)}} |
||
| |
| |
||
| Line 494: | Line 494: | ||
| |
| |
||
| |
| |
||
|[[ICP Etching Recipes#InP Ridge Etch .28Oxford ICP Etcher.29|R]] |
|||
|R |
|||
|{{rl|ICP Etching Recipes|ICP-Etch (Unaxis VLR)|InP-InGaAs-InAlAs Etch (Unaxis VLR)|InP Etch (Unaxis VLR)}} |
|{{rl|ICP Etching Recipes|ICP-Etch (Unaxis VLR)|InP-InGaAs-InAlAs Etch (Unaxis VLR)|InP Etch (Unaxis VLR)}} |
||
| |
| |
||
| Line 513: | Line 513: | ||
|A |
|A |
||
|A |
|A |
||
|[[ICP Etching Recipes#InP Ridge Etch .28Oxford ICP Etcher.29|R]] |
|||
|R |
|||
|{{rl|ICP Etching Recipes|ICP-Etch (Unaxis VLR)|InP-InGaAs-InAlAs Etch (Unaxis VLR)|InP Etch (Unaxis VLR)}} |
|{{rl|ICP Etching Recipes|ICP-Etch (Unaxis VLR)|InP-InGaAs-InAlAs Etch (Unaxis VLR)|InP Etch (Unaxis VLR)}} |
||
| |
| |
||
Revision as of 20:53, 8 October 2021
- R = Recipe is available. Clicking this link will take you to the recipe.
- A = Material is available for use, but no recipes are provided.