Resistivity Mapper (CDE RESMAP): Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
Millerski w (talk | contribs)
Updated SOP
Millerski w (talk | contribs)
Updated SOP
 
Line 19: Line 19:


*[[CDE ResMap Quick-Start instructions]]
*[[CDE ResMap Quick-Start instructions]]
*[https://wiki.nanofab.ucsb.edu/w/images/3/37/CDE_ResMap_Operating_Instructions.pdf CDE ResMap SOP]
*[https://wiki.nanofab.ucsb.edu/w/images/3/37/CDE_ResMap_Operating_Instructions.pdf CDE ResMap Operating Instructions]
*System can export CSV files - contact supervisor for instructions.
*System can export CSV files - contact supervisor for instructions.

Latest revision as of 22:07, 30 October 2023

Resistivity Mapper (CDE RESMAP)
Location Bay ?
Tool Type Inspection, Test and Characterization
Manufacturer Creative Design Engineering
Description CDE Resmap 4 Point Resistivity Mapper

Primary Supervisor Bill Millerski
(805) 893-2655
wmillerski@ucsb.edu

Secondary Supervisor

Tony Bosch


Recipes


About

The CDE Resmap 4 point resistivity mapper is used for measuring resistivity across the wafer for substrates and thin films deposited in the facility. The system can do automated resistivity mapping for pieces to 8 inch wafers.

The resistivity range is 2 mOhm/Square to 5 MOhm/square. Contour plots, 3D plots, histograms, data exporting are supported from the Windows XP based control system.

Instructions