=====Stepper #1 (GCA 6300) - Scheduled Maintenance=====
The tool will be undergoing maintenance and be unavailable the following dates and times:

1-18-24 at 8:00am to 1-18-24 at 6:00pm

Please plan your processing activities accordingly.

Bill Millerski

//[[User:Mehalana v|Vraj Mehalana]] 21:49, 21 December 2023 (PST)

===== Stepper #2 (GCA Autostep 200) - Scheduled Maintenance=====
The tool will be undergoing maintenance and be unavailable the following dates and times:

1-15-24 at 8:00am to 1-17-24 at 6:00pm

Please plan your processing activities accordingly.

//[[User:Mehalana v|Vraj Mehalana]] 21:49, 21 December 2023 (PST)

=====E-Beam #2 Heater is down - Update=====
=====E-Beam #2 Heater is down - Update=====
I am fairly certain the heater controller has failed. I have spoken with the vendor and they are looking into it, but we will most likely have to send the unit in. I will push to have a replacement controller sent instead, but since this is a warranty repair they will probably want to eval it in-house. I would plan for it to be down for at least a couple of weeks. I'll send out an update once I have more info.
I am fairly certain the heater controller has failed. I have spoken with the vendor and they are looking into it, but we will most likely have to send the unit in. I will push to have a replacement controller sent instead, but since this is a warranty repair they will probably want to eval it in-house. I would plan for it to be down for at least a couple of weeks. I'll send out an update once I have more info.

Revision as of 05:49, 22 December 2023

Stepper #1 (GCA 6300) - Scheduled Maintenance

The tool will be undergoing maintenance and be unavailable the following dates and times:

1-18-24 at 8:00am to 1-18-24 at 6:00pm

Please plan your processing activities accordingly.

Bill Millerski

//Vraj Mehalana 21:49, 21 December 2023 (PST)

Stepper #2 (GCA Autostep 200) - Scheduled Maintenance

The tool will be undergoing maintenance and be unavailable the following dates and times:

1-15-24 at 8:00am to 1-17-24 at 6:00pm

Please plan your processing activities accordingly.

//Vraj Mehalana 21:49, 21 December 2023 (PST)

E-Beam #2 Heater is down - Update

I am fairly certain the heater controller has failed. I have spoken with the vendor and they are looking into it, but we will most likely have to send the unit in. I will push to have a replacement controller sent instead, but since this is a warranty repair they will probably want to eval it in-house. I would plan for it to be down for at least a couple of weeks. I'll send out an update once I have more info.

//Vraj Mehalana 16:24, 14 December 2023 (PST)

DUV is down - Update

contacted our vendor for an update and was told that the parts should ship by this Friday. If all goes well the tool should be up mid next week.

//Vraj Mehalana 14:07, 13 December 2023 (PST)

PECVD2 Planned Down Time for Maintenance 12-11-23

PECVD2 will be going down on Monday 12-11-23 at 10:00am for replacement of the RF connector and RF Electrode.

When the work is complete, the process group will be running tests for the remainder of the afternoon.

//Vraj Mehalana 14:07, 13 December 2023 (PST)

Year End Shutdown

We will be shutting down lab operations Tuesday Dec 26th at 9 am for year end maintenance activities. The current plan is to be back open for operations Thursday Dec 28th at 2 pm. The staff will be on Holiday Dec 25th & 26th, and January 1st & 2nd.

//Vraj Mehalana 14:39, 16 November 2023 (PST)

Job Opening: Process Engineer

The Nanofab has a current job opening for a Process/Wafer-Fab Engineer, see the NanoFab Job Openings page for details.

//Vraj Mehalana 14:52, 30 October 2023 (PDT)

Lab Access Changes: Symmetry App

Card/Iris scanner access is still currently enabled. However we will be moving to a smartphone-based access system. IMPORTANT: check your email to setup the new smartphone access system, so you will be ready when we switch to the new system. Look for an email titled "Invitation to Access Symmetry App".

// John d 13:49, 7 November 2023 (PST)

Wafer Bonder, (Suss SB6-8E)

SUSS now aims to be on site in early February. I’ll will send out an email once I get confirmation for a specific date. //Vraj Mehalana 14:23, 13 December 2023 (PST)