Surface Analysis (KLA/Tencor Surfscan): Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Line 25: Line 25:
==Standard Recipes==
==Standard Recipes==


*[https://drive.google.com/drive/u/0/folders/135jBoHKLJ0uoLyD6NlHt_pgco8NJjdCs Standard Recipes]
*[https://wiki.nanotech.ucsb.edu/w/images/9/96/Surfscan-Operation-Manual.pdf Operations Manual]
*[https://wiki.nanotech.ucsb.edu/w/images/9/96/Surfscan-Operation-Manual.pdf Operations Manual]



Revision as of 22:45, 21 December 2023

Surface Analysis (KLA/Tencor Surfscan)
KLA.jpg
Location Bay 5
Tool Type Inspection, Test and Characterization
Manufacturer Tencor
Description Surface Analysis
KLA/Tencor Surfscan

Primary Supervisor Biljana Stamenic
(805) 893-4002
biljana@ece.ucsb.edu

Secondary Supervisor

Don Freeborn


Recipes


About

This system uses a laser-based scattering method to count size and distribution of particles (or other scattering defects) on a flat wafer surface. It can scan wafers in size from 4 to 8 inches.

Documentation

Standard Recipes

Examples


A low-particle 4-inch wafer example:
Gain 4: Small Particles

(0.160µm – 1.60µm)

Gain 2: Large Particles

(1.60µm – 28.0µm)

Surfscan Low-Particle Example - G4.png Surfscan Low-Particle Example - G2.png
A high-particle 4-inch wafer example:
Gain 4: Small Particles

(0.160µm – 1.60µm)

Gain 2: Large Particles

(1.60µm – 28.0µm)

Surfscan - 230113A7 Gain4 high particles.jpg Surfscan 230113A7G2 after low particles.jpg