Dry Etching Recipes: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
Did process rankings for ICP2, I also deleted a redundant row for Ru, there were two Ru rows |
added link to Al etch |
||
| Line 57: | Line 57: | ||
| |
| |
||
|{{rl|ICP Etching Recipes|Al Etch (Panasonic 1)}} |
|{{rl|ICP Etching Recipes|Al Etch (Panasonic 1)}} |
||
|[https://wiki.nanofab.ucsb.edu/wiki/ICP_Etching_Recipes#Al_Etch_.28Panasonic_2.29 R2] |
|||
|R2 |
|||
| |
| |
||
| |
| |
||
Revision as of 17:36, 30 July 2024
fProcess Control Data
See above linked page for process control data (dep rate/stress etc. over time), for a selection of often-used dry etches
Dry Etching Tools/Materials Table
The Key/Legend for this table's A...R6 values is at the bottom of the page.
Process Ranking Table
Processes in the table above are ranked by their "Process Maturity Level" as follows:
| Process Level | Description of Process Level Ranking | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| A | Process Allowed and materials available but never done | ||||||||||
| R1 | Process has been run at least once | ||||||||||
| R2 | Process has been run and/or procedure is documented or/and data available | ||||||||||
| R3 | Process has been run, procedure is documented, and data is available | ||||||||||
| R4 | Process has a documented procedure with regular (≥4x per year) data or lookahead/in-situ control available | ||||||||||
| R5 | Process has a documented procedure with regular (≥4x per year) data and lookahead/in-situ control available | ||||||||||
| R6 | Process has a documented procedure, regular ( ≥4x per year) data, and control charts & limits available | ||||||||||