Vacuum Deposition Recipes: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
R5 on IBD Al2O3 |
Add R level for UNAXIS PECVD |
||
| Line 593: | Line 593: | ||
|[[PECVD Recipes#SiN deposition .28PECVD .231.29|R6]] |
|[[PECVD Recipes#SiN deposition .28PECVD .231.29|R6]] |
||
|[[PECVD Recipes#SiN deposition .28PECVD .232.29|R6]] |
|[[PECVD Recipes#SiN deposition .28PECVD .232.29|R6]] |
||
| |
|[[PECVD Recipes#SiN 250C deposition .28Unaxis VLR.29|R6]] |
||
|<br> |
|<br> |
||
|<br> |
|<br> |
||
| Line 610: | Line 610: | ||
|[[PECVD Recipes#Low Stress Si3N4 .28PECVD.231.29|R4]] |
|[[PECVD Recipes#Low Stress Si3N4 .28PECVD.231.29|R4]] |
||
|[[PECVD Recipes#Low-Stress SiN deposition .28PECVD .232.29|R6]] |
|[[PECVD Recipes#Low-Stress SiN deposition .28PECVD .232.29|R6]] |
||
| |
|[[PECVD Recipes#SiN 250C deposition .28Unaxis VLR.29|R6]] |
||
| |
| |
||
| |
| |
||
| Line 627: | Line 627: | ||
| bgcolor="#eeffff" |[[PECVD Recipes#SiO2 deposition .28PECVD .231.29|R6]] |
| bgcolor="#eeffff" |[[PECVD Recipes#SiO2 deposition .28PECVD .231.29|R6]] |
||
| bgcolor="#eeffff" |[[PECVD Recipes#SiO2 deposition .28PECVD .232.29|R6]] |
| bgcolor="#eeffff" |[[PECVD Recipes#SiO2 deposition .28PECVD .232.29|R6]] |
||
| bgcolor="#eeffff" | |
| bgcolor="#eeffff" |[[PECVD Recipes#SiN 250C deposition .28Unaxis VLR.29|R6]] |
||
| bgcolor="#eeffff" |[[Atomic Layer Deposition Recipes#Pt deposition .28ALD CHAMBER 1.29|R4]] |
| bgcolor="#eeffff" |[[Atomic Layer Deposition Recipes#Pt deposition .28ALD CHAMBER 1.29|R4]] |
||
| bgcolor="#eeffff" |<br> |
| bgcolor="#eeffff" |<br> |
||
Revision as of 21:11, 31 July 2024
Process Control Data
See linked page for process control data (calibration data over time, such as dep. rate, refractive index, stress etc.) over time, for a selection of highly used tools/films.
Deposition Tools/Materials Table
- R: Recipe is available. Clicking this link will take you to the recipe.