Surface Analysis (KLA/Tencor Surfscan): Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
| Line 27: | Line 27: | ||
'' |
'' |
||
* Surfscan instructions [wafers different size, and pieces] |
* Surfscan instructions [wafers different size, and pieces] |
||
[[Surfscan SOP for small substrates]] |
|||
[[Surfscan SOP for 4inch wafers]] |
[[Surfscan SOP for 4inch wafers]] |
||
*[https://drive.google.com/drive/folders/1KfYJ4UcgIIlJof6tpLLz5wstzI7ureKx 8inch wafers] |
|||
Surfscan SOP for 6inch wafers |
|||
*[https://drive.google.com/drive/folders/1A-EOaVv7BZ7LqBU-ootweDXzz8KXIF3s 6inch wafers] |
|||
*[https://drive.google.com/drive/folders/1EUoxJusqM7We6EMnK64aG08ijyCjwt3U 4inch wafers] |
|||
Surfscan SOP for 8inch wafers |
|||
*[https://drive.google.com/drive/folders/1ypVvJM5PEay0fwscYaWHG53XlYlmpJUF All kind of small substrates] |
|||
**''You must water-mount your small sample or wafer(2inch or 3 inch) to a 4-inch wafer.'' |
**''You must water-mount your small sample or wafer(2inch or 3 inch) to a 4-inch wafer.'' |
||
*[[Wafer scanning process traveler|Wafer Particle Count - Process Traveler]]- Very detailed instructions |
*[[Wafer scanning process traveler|Wafer Particle Count - Process Traveler]]- Very detailed instructions |
||
Revision as of 22:56, 20 November 2024
| ||||||||||||||||||||||||||
About
This system uses a laser-based scattering method to count size and distribution of particles (or other scattering defects) on a flat wafer surface.
It can scan wafers in size from 4 to 8 inches. Piece-parts are more difficult but can be scanned with a custom recipe.
4-inch wafers are the most standard size to measure.
For measuring very low particle counts accurately, purchase "low particle count" (LPC) wafers from a Silicon wafer vendor, and keep the wafers in the case and clean at all times until use.
Documentation
Operating Procedures
- Wafer Scanning Instructions
- This is the procedure Staff uses to calibrate particle counts on our deposition tools. After the scan is complete you need to press ENTER on a small laptop. The Data will be saved on: Desktop/Local Disk(C)/Users/Public/Public Documentation] The data will be saved as a photo.
- Surfscan instructions [wafers different size, and pieces]
Surfscan SOP for small substrates
Surfscan SOP for 6inch wafers
Surfscan SOP for 8inch wafers
- You must water-mount your small sample or wafer(2inch or 3 inch) to a 4-inch wafer.
- Wafer Particle Count - Process Traveler- Very detailed instructions
Other Documentation
- Operations Manual
- For detailed measurement info, it is highly recommended that you read the manual.
Examples
| Gain 4: Small Particles
(0.160µm – 1.60µm) |
Gain 2: Large Particles
(1.60µm – 28.0µm) |
|---|---|
| Gain 4: Small Particles
(0.160µm – 1.60µm) |
Gain 2: Large Particles
(1.60µm – 28.0µm) |
|---|---|