Line 99: Line 99:
|7.20
|7.20
|0.305
|0.305
|
|155
|
|
|-
|-
Line 142: Line 142:
|0.381
|0.381
|
|
|
|-
|Indium
|In
|7.30
|0.841
|120
|
|
|-
|-