RIE Etching Recipes: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
| Line 4: | Line 4: | ||
==CdZnTe Etching (RIE 2)== |
==CdZnTe Etching (RIE 2)== |
||
*[[media:11-CZT_etching-1.pdf|CdZnTe Etch Recipes - CH<sub>4</sub>-H<sub>2</sub>-Ar]] |
*[[media:11-CZT_etching-1.pdf|CdZnTe Etch Recipes - CH<sub>4</sub>-H<sub>2</sub>-Ar]] |
||
==ITO Etching (RIE 2)== |
|||
*[[media:RIE2-ITO-Etch-MHA-Plasma-RevA.pdf|ITO Etch Recipes - CH<sub>4</sub>-H<sub>2</sub>-Ar]] |
|||
==InP-InGaAsP-InGaAlAs Etching (RIE 2)== |
==InP-InGaAsP-InGaAlAs Etching (RIE 2)== |
||