Tube Furnace (Tystar 8300): Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
Bosch (talk | contribs)
Bosch (talk | contribs)
Line 22: Line 22:


Use the BYU Thermal Oxidation Calculator to determine the time and temperature that will be necessary for your process needs. Keep in mind that all process must be 30 minutes in length at a minimum. Processes less than 30 minutes will suffer from poor uniformity because the process tube will not have sufficient time to saturate with O<sub>2</sub> or DI-H<sub>2</sub>O.
Use the BYU Thermal Oxidation Calculator to determine the time and temperature that will be necessary for your process needs. Keep in mind that all process must be 30 minutes in length at a minimum. Processes less than 30 minutes will suffer from poor uniformity because the process tube will not have sufficient time to saturate with O<sub>2</sub> or DI-H<sub>2</sub>O.

http://www.cleanroom.byu.edu/OxideTimeCalc.phtml


=Recipes=
=Recipes=

Revision as of 20:46, 18 March 2014

Tube Furnace (Tystar 8300)
Tool Type Thermal Processing
Location Bay 4
Supervisor Tony Bosch
Supervisor Phone (805) 893-3486
Supervisor E-Mail bosch@ece.ucsb.edu
Description Tystar 8" 3-Tube Oxidation/Annealing System
Manufacturer Tystar Corporation
Sign up for this tool


About

The three stack Tystar 8” furnace is used primarily for 3 processes. The processes are dedicated for one tube each:

  1. SOG curing - Tube 1
  2. Dry or wet oxidation of silicon - Tubes 2 and 3
  3. General furnace annealing - Tube 3

Each process tube can accomodate up to one hundred 8” wafers per cycle. We have boats for 2", 3", 4", 6", 8" and irregular shaped pieces. The maximum temperature is 1050°C for the system. Gases used are O2, Steam from DI-H2O, N2.

Process Information

Use the BYU Thermal Oxidation Calculator to determine the time and temperature that will be necessary for your process needs. Keep in mind that all process must be 30 minutes in length at a minimum. Processes less than 30 minutes will suffer from poor uniformity because the process tube will not have sufficient time to saturate with O2 or DI-H2O.

Recipes

Tube 1 - SOG425.001

Tube 2 - WET1050.002, DRY1050.002, WETVAR.002, DRYVAR.002

Tube 3 - WET1050.003, DRY1050.003, WETVAR.003, DRYVAR.003, ANNEAL.003