* [[media:PECVD1-SiON-Recipe.pdf|Low Stress Si<sub>3</sub>N<sub>4</sub> - Variable Stress Plot]]
* [[media:PECVD1-SiON-Recipe.pdf|Low Stress Si<sub>3</sub>N<sub>4</sub> - Variable Stress Plot]]


*Deposition rate~11.23nm/min (users must calibrate this prior to critical deps)
*Deposition rate~11.21nm/min (users must calibrate this prior to critical deps)
*HF e.r.~89nm/min
*HF e.r.~89nm/min
*Stress~450MPa
*Stress~447MPa
*Refractive Index~1.942
*Refractive Index~1.942