* [[media:PECVD1-SiON-Recipe.pdf|Low Stress Si<sub>3</sub>N<sub>4</sub> - Variable Stress Recipes]]
* [[media:PECVD1-SiON-Recipe.pdf|Low Stress Si<sub>3</sub>N<sub>4</sub> - Variable Stress Recipes]]
* [[media:PECVD1-SiON-Recipe.pdf|Low Stress Si<sub>3</sub>N<sub>4</sub> - Variable Stress Plot]]
* [[media:PECVD1-SiON-Recipe.pdf|Low Stress Si<sub>3</sub>N<sub>4</sub> - Variable Stress Plot]]

== LS SiO<sub>x</sub>N<sub>y</sub> deposition (PECVD #1) ==
<!-- Placeholders - Not uploaded yet-->
*[[media:PECVD1-SiON-Recipe.pdf|SiO<sub>x</sub>N<sub>y</sub> Deposition Recipes - Varying N/O Ratio]]
*[[media:PECVD1-SiON-Plot.pdf|SiO<sub>x</sub>N<sub>y</sub> Stress/Index vs. O/N Ratio]]
*[[media:PECVD1-LS SION recipe 2014.pdf|SiO<sub>x</sub>N<sub>y</sub> Recipe]]
*[https://docs.google.com/spreadsheets/d/1rixyzAAq6q08M5OwvZiDVoh3K8B566XKM-UZAQIAnsg/edit#gid=sharing SiO<sub>x</sub>N<sub>y</sub> Data December 2014]
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dEttR2JSTkRoamR0SUZ4bE5QUW9uS2c&usp=sharing SiO<sub>x</sub>N<sub>y</sub> 3000A Thickness uniformity 2014]


== LS SiN deposition (PECVD #1) ==
== LS SiN deposition (PECVD #1) ==