Template:Announcements: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
removed ICP#1 |
|||
| Line 18: | Line 18: | ||
// [[User:John d|Posted:]] 13:07, 11 December 2017 (PST) |
// [[User:John d|Posted:]] 13:07, 11 December 2017 (PST) |
||
===== |
===== Cary 500 ===== |
||
Pump failed. Don is installing a replacement. |
|||
| ⚫ | |||
// [[User:John d|Posted:]] 15:06, 7 December 2017 (PST) |
// [[User:John d|Posted:]] 15:06, 7 December 2017 (PST) |
||
===== GCA 6300 Stepper #1 ===== |
===== GCA 6300 Stepper #1 ===== |
||
Lamp power supply has been replaced. |
Lamp power supply has been replaced. |
||
// [[User:John d|Posted:]] 16:31, 11 December 2017 (PST) |
// [[User:John d|Posted:]] 16:31, 11 December 2017 (PST) |
||
===== Cary 500 ===== |
|||
| ⚫ | |||
// [[User:John d|Posted:]] 15:06, 7 December 2017 (PST) |
|||
<!---------- end of announcements ------------> |
<!---------- end of announcements ------------> |
||
Revision as of 01:21, 13 December 2017
Announcements
// The NanoFab is Open.
// The Thomas Fire has caused repeated power outages since the evening of Monday 12/4. CalFire is posting updates on their webpage and FaceBook page.
// Posted: 13:07, 11 December 2017 (PST)
Cary 500
UV-Vis Detector Failure. Locating replacement. // Posted: 15:06, 7 December 2017 (PST)
GCA 6300 Stepper #1
Lamp power supply has been replaced. // Posted: 16:31, 11 December 2017 (PST)