CDE ResMap Quick-Start instructions: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
initial instrucitons
 
photo of measurement locations
 
Line 4: Line 4:
## Programs for Quarter wafers will measure opposite the white stick. See image below.
## Programs for Quarter wafers will measure opposite the white stick. See image below.
## You can always load a 6" wafer (eg. from teh discarded ICP carriers) and run a program to see where it is going to measure.
## You can always load a 6" wafer (eg. from teh discarded ICP carriers) and run a program to see where it is going to measure.
{| class="wikitable"
|+Measurement locations for Full- and Quarter-Wafer programs
![[File:CDE ResMap Full Wafer meas location - IMG 0112 - 800px annot.png|none|thumb|200x200px|Full Wafer centered on stage]]
![[File:CDE ResMap Quarter Wafer meas location - 800px annot quarterwf.png|none|thumb|200x200px|Quarter Wafer recipe measurement location]]
|}

== Quick Measurement Procedure ==
# Select Operator > Run Recipe
# Select Operator > Run Recipe
# Choose a recipe in "UCSB Users"
# Choose a recipe in "UCSB Users"

Latest revision as of 20:01, 17 April 2018

  1. Depending on the program you run, your sample location may be different.
    1. In general, programs for full 4-inch wafers require the wafer to be centered on the stage.
    2. Wafer flat should face the white sticker on the stage.
    3. Programs for Quarter wafers will measure opposite the white stick. See image below.
    4. You can always load a 6" wafer (eg. from teh discarded ICP carriers) and run a program to see where it is going to measure.
Measurement locations for Full- and Quarter-Wafer programs
Full Wafer centered on stage
Quarter Wafer recipe measurement location

Quick Measurement Procedure

  1. Select Operator > Run Recipe
  2. Choose a recipe in "UCSB Users"
    1. Filename indicates whether it will measure a Full or quarter wafer, number of points, wafer diameter etc.
  3. Choose a "Filename" for your data. Enable "Auto Plot" to show a contour plot.
  4. [Run] to perform the scan.
    1. You can Abort the scan by pressing Any key, and click [Abort] at the top.
  5. Sheet resistance of every measured point is shown on the next screen.
    1. "Rs" is sheet resistance, "RsAvg" is Average of all measured points.