Dry Etching Recipes: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
renamed/linked SiDeepRIE → SLR Fluorine ICP |
m replace bottom link from SiDeepEtch → SLR Fluorine ICP |
||
| Line 755: | Line 755: | ||
| bgcolor="#daf1ff" | [[RIE_Etching_Recipes#RIE_5_.28PlasmaTherm.29|RIE 5<br>(PlasmaTherm)]] |
| bgcolor="#daf1ff" | [[RIE_Etching_Recipes#RIE_5_.28PlasmaTherm.29|RIE 5<br>(PlasmaTherm)]] |
||
| bgcolor="#daf1ff" | [[ICP_Etching_Recipes#DSEIII_.28PlasmaTherm.2FDeep_Silicon_Etcher.29|DSEIII<br>(PlasmaTherm)]] |
| bgcolor="#daf1ff" | [[ICP_Etching_Recipes#DSEIII_.28PlasmaTherm.2FDeep_Silicon_Etcher.29|DSEIII<br>(PlasmaTherm)]] |
||
| bgcolor="#daf1ff" | [[ |
| bgcolor="#daf1ff" | [[Fluorine ICP Etcher (PlasmaTherm/SLR Fluorine ICP)|SLR Fluorine ICP (PlasmaTherm)]] |
||
| bgcolor="#daf1ff" | [[ICP_Etching_Recipes#ICP_Etch_1_.28Panasonic_E626I.29|ICP Etch 1<br>(Panasonic E626I)]] |
| bgcolor="#daf1ff" | [[ICP_Etching_Recipes#ICP_Etch_1_.28Panasonic_E626I.29|ICP Etch 1<br>(Panasonic E626I)]] |
||
| bgcolor="#daf1ff" | [[ICP_Etching_Recipes#ICP_Etch_2_.28Panasonic_E640.29|ICP Etch 2<br>(Panasonic E640)]] |
| bgcolor="#daf1ff" | [[ICP_Etching_Recipes#ICP_Etch_2_.28Panasonic_E640.29|ICP Etch 2<br>(Panasonic E640)]] |
||
Revision as of 22:20, 28 August 2018
- R = Recipe is available. Clicking this link will take you to the recipe.
- A = Material is available for use, but no recipes are provided.