ICP-PECVD (Unaxis VLR): Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
added cluster configuration / link to each chamber's tool page |
|||
| Line 11: | Line 11: | ||
|toolid=17 |
|toolid=17 |
||
}} |
}} |
||
= |
=About= |
||
This system is configured as an ICP PECVD deposition tool with 1000 W ICP power, 600 W RF substrate power, and 50°C-350°C operation. This chamber has 100% SiH<sub>4,</sub> N<sub>2</sub>, O<sub>2</sub>, and Ar for gas sources. The high density PECVD produces a more dense, higher quality SiO<sub>2</sub> and Si<sub>3</sub>N<sub>4</sub>, as compared with conventional PECVD. With the high density plasma, deposition of high quality films can be deposited as low as 50°C for processes requiring lower temperatures. Stress compensation for silicon nitride is characterized. |
This system is configured as an ICP PECVD deposition tool with 1000 W ICP power, 600 W RF substrate power, and 50°C-350°C operation. This chamber has 100% SiH<sub>4,</sub> N<sub>2</sub>, O<sub>2</sub>, and Ar for gas sources. The high density PECVD produces a more dense, higher quality SiO<sub>2</sub> and Si<sub>3</sub>N<sub>4</sub>, as compared with conventional PECVD. With the high density plasma, deposition of high quality films can be deposited as low as 50°C for processes requiring lower temperatures. Stress compensation for silicon nitride is characterized. |
||
=== Cluster Configuration === |
|||
| ⚫ | |||
A Deposition and Etch chamber are both attached to the same loadlock, allowing etching and deposition without breaking vacuum. Each chamber can be scheduled separately on SignupMonkey. |
|||
* PM3: [[ICP-PECVD (Unaxis VLR)|ICP-PECVD Deposition (Unaxis VLR)]] |
|||
* PM1: [[ICP-Etch (Unaxis VLR)|ICP Etch (Unaxis VLR)]] |
|||
| ⚫ | |||
*1000W ICP source, 600W RF Sample Bias Power Supply |
*1000W ICP source, 600W RF Sample Bias Power Supply |
||
| Line 23: | Line 29: | ||
=Documentation= |
=Documentation= |
||
*[ |
*[//www.nanotech.ucsb.edu/wiki/images/1/1f/Unaxis_PM3_Web_Operational_Procedure_3-27-14.pdf Operating Instructions] |
||
Revision as of 22:23, 27 November 2019
| |||||||||||||||||||||
About
This system is configured as an ICP PECVD deposition tool with 1000 W ICP power, 600 W RF substrate power, and 50°C-350°C operation. This chamber has 100% SiH4, N2, O2, and Ar for gas sources. The high density PECVD produces a more dense, higher quality SiO2 and Si3N4, as compared with conventional PECVD. With the high density plasma, deposition of high quality films can be deposited as low as 50°C for processes requiring lower temperatures. Stress compensation for silicon nitride is characterized.
Cluster Configuration
A Deposition and Etch chamber are both attached to the same loadlock, allowing etching and deposition without breaking vacuum. Each chamber can be scheduled separately on SignupMonkey.
Detailed Specifications
- 1000W ICP source, 600W RF Sample Bias Power Supply
- 50 - 350°C sample temperature
- 100% SiH4, Ar, N2, O2
- Multiple 4” diameter wafer capable system
- Pieces possible by mounting or placing on 4 ” wafer