WIP.... |
WIP.... |
||
The wafers for process calibration are ordered from SVM (<nowiki>https://www.svmi.com/</nowiki>). These are: 4” Si wafers, P/Boron, <100>, 1-30 ohm-cm, 525 +/-25 microns, Polished/Etched, Particles: <=10 @ >=0.3 microns, and have low LPD count (LPD= light particle detection, LPD<100). |
|||
=== Scan before process calibration === |
|||
Revision as of 17:39, 20 April 2020
WIP....
The wafers for process calibration are ordered from SVM (https://www.svmi.com/). These are: 4” Si wafers, P/Boron, <100>, 1-30 ohm-cm, 525 +/-25 microns, Polished/Etched, Particles: <=10 @ >=0.3 microns, and have low LPD count (LPD= light particle detection, LPD<100).