PECVD 2 (Advanced Vacuum): Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
| Line 37: | Line 37: | ||
* |
* |
||
* |
* |
||
* [ |
* [https://wiki.nanotech.ucsb.edu/w/images/2/2c/SOP_for_Advanced_Vacuum_PECVD.pdf Operating Instructions for Adv. PECVD II] |
||
* [[Wafer Coating Process Traveler]] |
* [[Wafer Coating Process Traveler]] |
||
* For particle counting method, see the [[Wafer scanning process traveler|Surfscan Scanning Procedure]] |
* For particle counting method, see the [[Wafer scanning process traveler|Surfscan Scanning Procedure]] |
||
Revision as of 17:12, 27 May 2020
| |||||||||||||||||||||
About
This open-load system is dedicated to PECVD of SiO2, SiNx, SiOxNy, and a-Si using Silane (2%SiH4, 98% He), N2O, NH3, and N2 gases. The sample electrode has a 270mm diameter useable area, allowing for multiple 4” wafer depositions in a single run. Standard operating temperature is 300C, but can be user changed for temps ranging anywhere from 250 to 350C. The system is equipped with a dual generator, dual frequency option for growth of low-stress Nitride films.
Recipes
- Recipes for SiO2, Si3N4 and Low-Stress Si3N4 can be found on the PECVD Recipes Page:
- A list of all available deposited films can be found on the Vacuum Deposition Recipes page: