detailed specs - first pass
note that DUV camera is non-funcitonal
Line 10: Line 10:
|model= MX61A-DUV
|model= MX61A-DUV
}}
}}
'''DUV Camera is non-operational and unable to be repaired. Visible camera is still functional. 2022-02'''
⚫
== About ==

⚫
==About==
This system does general purpose imaging in the visible and also has high resolution/high magnification DUV imaging using 250 nm light. Surface features less than 100nm can be resolved.
This system does general purpose imaging in the visible and also has high resolution/high magnification DUV imaging using 250 nm light. Surface features less than 100nm can be resolved.


Line 17: Line 19:
A Good system for CD measurements on wafer (250nm and above) without entry into the SEM.
A Good system for CD measurements on wafer (250nm and above) without entry into the SEM.


== Detailed Specifications ==
==Detailed Specifications==
⚫
* Microscope Objectives:
⚫
** 5x, 10x, 20x, 50x, 100x, DUV-100x
⚫
* Software Control:
⚫
** Motorized Stage & Objective Turret
⚫
** Calibrated Measurements (calibrations fixed)
⚫
** Z-motor (focus height) measurement
⚫
* Filters:
⚫
** Bright Field / Dark Field (visible only)


⚫
*Microscope Objectives:
⚫
== Examples ==
⚫
**5x, 10x, 20x, 50x, 100x, DUV-100x
⚫
*Software Control:
⚫
**Motorized Stage & Objective Turret
⚫
**Calibrated Measurements (calibrations fixed)
⚫
**Z-motor (focus height) measurement
⚫
*Filters:
⚫
**Bright Field / Dark Field (visible only)

⚫
==Examples==
[[File:Olympus MX61A-DUV res test 100x DUV v1.png|alt=DUV microscope image with 1µm scale bar|none|thumb|504x504px|100x DUV image taken with the Olympus MX61A-DUV, showing sub-micron resolution.]]
[[File:Olympus MX61A-DUV res test 100x DUV v1.png|alt=DUV microscope image with 1µm scale bar|none|thumb|504x504px|100x DUV image taken with the Olympus MX61A-DUV, showing sub-micron resolution.]]

== Other Info ==
'''''Equip > Characterization > [[Microscopes]]''''' - ''see a list of all our microscopes''

Revision as of 17:27, 6 June 2022

Deep UV Optical Microscope (Olympus)
Tool Type Inspection, Test and Characterization
Location Bay 7
Supervisor Tony Bosch
Supervisor Phone (805) 893-3486
Supervisor E-Mail bosch@ece.ucsb.edu
Description Deep-Ultraviolet (250nm) Microscope
Manufacturer Olympus
Model MX61A-DUV


DUV Camera is non-operational and unable to be repaired. Visible camera is still functional. 2022-02

About

This system does general purpose imaging in the visible and also has high resolution/high magnification DUV imaging using 250 nm light. Surface features less than 100nm can be resolved.

The system has precision motorized stage control and is fully computer controlled for image capture and sample manipulation.

A Good system for CD measurements on wafer (250nm and above) without entry into the SEM.

Detailed Specifications

  • Microscope Objectives:
    • 5x, 10x, 20x, 50x, 100x, DUV-100x
  • Software Control:
    • Motorized Stage & Objective Turret
    • Calibrated Measurements (calibrations fixed)
    • Z-motor (focus height) measurement
  • Filters:
    • Bright Field / Dark Field (visible only)

Examples

DUV microscope image with 1µm scale bar
100x DUV image taken with the Olympus MX61A-DUV, showing sub-micron resolution.

Other Info

Equip > Characterization > Microscopes - see a list of all our microscopes