Dry Etching Recipes: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
mention + link to table Key/Legend |
|||
| Line 1: | Line 1: | ||
===<u>[[Process Group - Process Control Data#Etching .28Process Control Data.29|Process Control Data]]</u>=== |
===<u>[[Process Group - Process Control Data#Etching .28Process Control Data.29|Process Control Data]]</u>=== |
||
<small>''See [[Process Group - Process Control Data#Etching .28Process Control Data.29|linked page]] for [https://en.wikipedia.org/wiki/Statistical_process_control process control data] (dep rate/stress etc. over time), for a selection of often-used |
<small>''See above [[Process Group - Process Control Data#Etching .28Process Control Data.29|linked page]] for [https://en.wikipedia.org/wiki/Statistical_process_control process control data] (dep rate/stress etc. over time), for a selection of often-used dry etches''</small> |
||
===Dry Etching Tools/Materials Table=== |
===Dry Etching Tools/Materials Table=== |
||
''The Key/Legend for this table's <code>A...R5</code> values is at the [[Dry Etching Recipes#Process Ranking Table|bottom of the page]].'' |
|||
{| class="wikitable" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center; font-size: 95%" border="1" |
{| class="wikitable" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center; font-size: 95%" border="1" |
||
|- |
|- |
||
Revision as of 16:30, 24 July 2024
Process Control Data
See above linked page for process control data (dep rate/stress etc. over time), for a selection of often-used dry etches
Dry Etching Tools/Materials Table
The Key/Legend for this table's A...R5 values is at the bottom of the page.
Process Ranking Table
| Process Level | Description of Process Level Ranking | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| A | Process allowed and materials available but never done | ||||||||||
| R1 | Process has been ran at least once | ||||||||||
| R2 | Process has been ran and/or procedure is documented or/and data available | ||||||||||
| R3 | Process has been ran, procedure is documented, and data is available | ||||||||||
| R4 | Process has a documented procedure with regular (≥4x per year) data or lookahead/in-Situ control available | ||||||||||
| R5 | Process has a documented procedure with regular (≥4x per year) data and lookahead/in-Situ control available | ||||||||||