Dry Etching Recipes: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
changed PR/BARC etch and SiN etch on FICP to R3 |
changed Ru etch on ICP2 to R3 |
||
| Line 212: | Line 212: | ||
| |
| |
||
|A |
|A |
||
|[https://wiki.nanofab.ucsb.edu/wiki/ICP_Etching_Recipes#Ru_.28Ruthenium.29_Etch_.28Panasonic_2.29 |
|[https://wiki.nanofab.ucsb.edu/wiki/ICP_Etching_Recipes#Ru_.28Ruthenium.29_Etch_.28Panasonic_2.29 R3] |
||
| |
| |
||
| |
| |
||
Revision as of 17:40, 9 August 2024
Process Control Data
See above linked page for process control data (dep rate/stress etc. over time), for a selection of often-used dry etches
Dry Etching Tools/Materials Table
The Key/Legend for this table's A...R6 values is at the bottom of the page.
Process Ranking Table
Processes in the table above are ranked by their "Process Maturity Level" as follows:
| Process Level | Description of Process Level Ranking | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| A | Process Allowed and materials available but never done | ||||||||||
| R1 | Process has been run at least once | ||||||||||
| R2 | Process has been run and/or procedure is documented or/and data available | ||||||||||
| R3 | Process has been run, procedure is documented, and data is available | ||||||||||
| R4 | Process has a documented procedure with regular (≥4x per year) data or lookahead/in-situ control available | ||||||||||
| R5 | Process has a documented procedure with regular (≥4x per year) data and lookahead/in-situ control available | ||||||||||
| R6 | Process has a documented procedure, regular ( ≥4x per year) data, and control charts & limits available | ||||||||||