=Detailed Specifications= |
|||
*Standard 18" bell jar pumped by 8" Varian cryopump (HV8) driven by Ebara 2.1 compressor |
|||
*Low E-7 Torr ultimate pressure |
|||
*Rate Monitor: Maxtek TM-300 |
|||
*Typical material rates: Al - 1 A/s @ 85 amps |
|||
**Au - 5 A/s @ 122 amps |
|||
**Cr - 2 A/s @ 85 amps |
|||
**Zn - 4.5 A/s @ 50 amps |
|||
= Materials Table = |
= Materials Table = |
||
Revision as of 23:08, 28 August 2012
| |||||||||||||||||||||
About
Materials Table
Materials Table
| |||||||
|---|---|---|---|---|---|---|---|
| Material | Symbol | Density, g/cm3 | Z Ratio | Tooling, % | Current, Amp | Dep.rate, A/sec | Comments |