PECVD Recipes: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
| Line 35: | Line 35: | ||
*[[Media:PECVD2-SiN-Recipe-50W-100C-Medium-Stress.pdf|SiN Deposition Recipe (50W 100° Medium Stress)]] |
*[[Media:PECVD2-SiN-Recipe-50W-100C-Medium-Stress.pdf|SiN Deposition Recipe (50W 100° Medium Stress)]] |
||
*[[Media:PECVD2-SiN-Recipe-120W-100C-Low-Stress.pdf|SiN Deposition Recipe (120W 100° Low Stress)]] |
*[[Media:PECVD2-SiN-Recipe-120W-100C-Low-Stress.pdf|SiN Deposition Recipe (120W 100° Low Stress)]] |
||
*[[Media:PECVD2-SiNx-Comparison table-2% SiH4-100C-120W.pdf| |
*[[Media:PECVD2-SiNx-Comparison table-2% SiH4-100C-120W.pdf|Comparison Table SiNx (120W 100° Low Stress)]] |
||
| |
| |
||
*[[Media:PECVD2-SiN-Recipe-5W-250C-High-Stress.pdf|SiN Deposition Recipe (5W 250° High Stress)]] |
*[[Media:PECVD2-SiN-Recipe-5W-250C-High-Stress.pdf|SiN Deposition Recipe (5W 250° High Stress)]] |
||
*[[Media:PECVD2-SiN-Recipe-50W-250C-Medium-Stress.pdf|SiN Deposition Recipe (50W 250° Medium Stress)]] |
*[[Media:PECVD2-SiN-Recipe-50W-250C-Medium-Stress.pdf|SiN Deposition Recipe (50W 250° Medium Stress)]] |
||
*[[Media:PECVD2-SiN-Recipe-120W-250C-Low-Stress.pdf|SiN Deposition Recipe (120W 250° Low Stress)]] |
*[[Media:PECVD2-SiN-Recipe-120W-250C-Low-Stress.pdf|SiN Deposition Recipe (120W 250° Low Stress)]] |
||
*[[Media:PECVD2-SiNx-Comparison table-2% SiH4-250C-120W.pdf| |
*[[Media:PECVD2-SiNx-Comparison table-2% SiH4-250C-120W.pdf|Comparison Table SiNx (120W 250° Low Stress)]] |
||
|- |
|- |
||
|} |
|} |
||
Revision as of 22:46, 3 October 2012
Back to Vacuum Deposition Recipes.
PECVD 1 (PlasmaTherm 790)
SiN deposition (PECVD #1)
SiO2 deposition (PECVD #1)
PECVD 2 (Advanced Vacuum)
SiN deposition (PECVD #2)
SiO2 deposition (PECVD #2)
ICP-PECVD (Unaxis VLR)
SiN deposition (Unaxis VLR)
SiN (2% SiH4)
| 50° | 100° | 250° |
|---|---|---|
SiN (2% SiH4 - No-Ar)
| 50° | 100° | 250° |
|---|---|---|
SiN (2% SiH4 - No-Ar - Extra N2)
| 50° | 100° | 250° |
|---|---|---|
SiN (100% SiH4 )
| 50° | 100° | 250° | |
|---|---|---|---|
SiO2 deposition (Unaxis VLR)
SiO2 (2% SiH4)
| 50° | 100° | 250° |
|---|---|---|
SiO2 (2% SiH4 - No Ar)
| 50° | 100° | 250° |
|---|---|---|
SiO2 (100% SiH4 HDR)
| 50° | 100° | 250° |
|---|---|---|
SiO2 (100% SiH4 LDR)
| 50° | 100° | 250° |
|---|---|---|