PECVD Recipes: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
| Line 3: | Line 3: | ||
== SiN deposition (PECVD #1) == |
== SiN deposition (PECVD #1) == |
||
*[[media:PECVD1-SiN-Recipe.pdf|SiN Deposition Recipe]] |
*[[media:PECVD1-SiN-Recipe.pdf|SiN Deposition Recipe]] |
||
*[[media:PECVD1-SiN-Data.pdf|SiN particle data]] |
|||
*[[media:PECVD1-WIKI PECVD SiN Index, dep.rates, stress.pdf| SIN data]] |
*[[media:PECVD1-WIKI PECVD SiN Index, dep.rates, stress.pdf| SIN data]] |
||
<!-- Placeholders - Not uploaded yet--> |
<!-- Placeholders - Not uploaded yet--> |
||
Revision as of 17:10, 11 September 2013
Back to Vacuum Deposition Recipes.
PECVD 1 (PlasmaTherm 790)
SiN deposition (PECVD #1)
- SiN Deposition Recipe
- SIN data
- Low Stress Si3N4 - Variable Stress Recipes
- Low Stress Si3N4 - Variable Stress Plot
SiO2 deposition (PECVD #1)
SiOxNy deposition (PECVD #1)
PECVD 2 (Advanced Vacuum)
SiN deposition (PECVD #2)
SiO2 deposition (PECVD #2)
ICP-PECVD (Unaxis VLR)
SiN deposition (Unaxis VLR)
SiN (2% SiH4)
SiN (2% SiH4 - No-Ar)
| 50° | 100° | 250° |
|---|---|---|
SiN (2% SiH4 - No-Ar - Extra N2)
| 50° | 100° | 250° |
|---|---|---|
SiN (100% SiH4 )
| 50° | 100° | 250° |
|---|---|---|
SiO2 deposition (Unaxis VLR)
SiO2 (2% SiH4)
| 50° | 100° | 250° |
|---|---|---|
SiO2 (2% SiH4 - No Ar)
| 50° | 100° | 250° |
|---|---|---|
SiO2 (100% SiH4 HDR)
| 50° | 100° | 250° |
|---|---|---|
SiO2 (100% SiH4 LDR)
| 50° | 100° | 250° |
|---|---|---|
Amorphous Si (100%SiH4 Ar He)
| 90° | 250° |
|---|---|