Mechanical Polisher (Allied)

From UCSB Nanofab Wiki
Revision as of 22:59, 24 October 2022 by John d (talk | contribs) (update to {{tool2}}, set Room = 1111)
Jump to navigation Jump to search
Mechanical Polisher (Allied)
Location ESB Rm. 1111
Tool Type Wet Processing
Manufacturer Allied High Tech Products Inc.
Model 10-1110
Description Mechanical Polisher

Primary Supervisor Bill Millerski
(805) 893-2655
wmillerski@ucsb.edu

Recipes

SignupMonkey: Sign up for this tool


About

The Allied Polisher allows for bulk thinning of substrates, and fine polishing of optical waveguide facets. Various materials are typically lapped/polished, such as Silicon GaAs, InP.

Detailed Specs

  • Max. Substrate Size
  • Lapping Films available:
    • 10µm AlOx
    • 5µm AlOx
    • 2µm AlOx
    • 1µm AlOx
    • 0.5 AlOx

Operating Procedures

  • To Be Added

Recipes

  • To Be Added