R
= Recipe is available. Clicking this link will take you to the recipe.
A
= Material is available for use, but no recipes are provided.
Dry Etching Recipes
RIE Etching
ICP Etching
Oxygen Plasma Systems
Other Dry Etchers
Material
RIE 2
(MRC)
RIE 3
(MRC)
RIE 5
(PlasmaTherm)
DSEIII
(PlasmaTherm)
Fluorine ICP
(PlasmaTherm)
ICP Etch 1
(Panasonic E626I)
ICP Etch 2
(Panasonic E640)
Oxford ICP
(PlasmaPro 100)
ICP-Etch
(Unaxis VLR)
Ashers
(Technics PEII)
Plasma Clean
(Gasonics 2000)
Plasma Clean
(YES EcoClean)
UV Ozone Reactor
Plasma Activation
(EVG 810)
XeF2 Etch
(Xetch)
Vapor HF Etch
(uETCH)
CAIBE
(Oxford)
Ag
A
Al
A
R1
R1
A
Au
R1
Cr
A
R1
A
A
Cu
A
Ge
A
A
A
A
Mo
A
Nb
A
A
Ni
R1
Os
A
A
Pt
R1
Ru
A
R1
A
Si
R1
R1
A
R1
A
Ta
A
A
A
Ti
R1
A
A
Al
2
O
3
R
A
Al
2
O
3 (Sapphire)
R1
A
A
AlGaAs
R1
R1
R
GaAs-AlGaAs Etch (Unaxis VLR)
A
AlGaN
R
R1
A
AlN
R1
A
CdZnTe
R1
A
GaAs
R1
R1
R1
R
GaAs-AlGaAs Etch (Unaxis VLR)
A
GaN
R1
R1
A
R
R1
A
GaSb
A
GaSb Etch Unaxis VLR)
A
HfO
2
A
InGaAlAs
InP-InGaAsP-InGaAlAs Etching (RIE 2)
A
InP-InGaAs-InAlAs Etch (Unaxis VLR)
A
InGaAsP
InP-InGaAsP-InGaAlAs Etching (RIE 2)
R
InP-InGaAs-InAlAs Etch (Unaxis VLR)
A
InP
InP-InGaAsP-InGaAlAs Etching (RIE 2)
A
A
R
InP-InGaAs-InAlAs Etch (Unaxis VLR)
R1
ITO
R1
A
Photoresist
& ARC
A
R
R
R
R
A
A
A
A
Ru
A
R
SiC
R1
A
A
SiN
SiN
x
Etching (RIE 3)
A
R1
R1
A
A
SiO
2
SiO
2
Etching (RIE 3)
R1
R1
R1
R1
A
SiOxNy
A
A
A
Ta
2
O
5
A
A
TiN
A
TiO
2
A
W-TiW
R1
A
A
ZnO
2
A
ZnS
R1
A
ZnSe
R1
A
ZrO
2
A
Material
RIE 2
(MRC)
RIE 3
(MRC)
RIE 5
(PlasmaTherm)
DSEIII
(PlasmaTherm)
Fluorine ICP
(PlasmaTherm)
ICP Etch 1
(Panasonic E626I)
ICP Etch 2
(Panasonic E640)
Oxford ICP
(PlasmaPro 100)
ICP-Etch
(Unaxis VLR)
Ashers
(Technics PEII)
Plasma Clean
(Gasonics 2000)
Plasma Clean
(YES EcoClean)
UV Ozone Reactor
Plasma Activation
(EVG 810)
XeF2 Etch
(Xetch)
Vapor HF Etch
(uETCH)
CAIBE
(Oxford)
Category
:
Processing
Navigation menu
Personal tools
Create account
Log in
Namespaces
Page
Discussion
English
Views
Read
View source
View history
More
Search
InvisibleMenu
QuickLinks
Lab Rules
Common Questions/FAQ
Staff List
Equipment Signup
Chemicals + MSDS
Protofab
Equipment
Full Tool List
Lithography
Vacuum Deposition
Dry Etch
Wet Processing
Thermal Processing
Packaging
Metrology & Test
Recipes and Data
Lithography
Vacuum Deposition
Dry Etching
Wet Etching
Thermal Processing
Packaging Tools
Data + Info
Process Control Data
Tutorials
Calculators/Utilities
NanoFab Info
Research + Pubs
Tech Talks
Tools
What links here
Related changes
Special pages
Printable version
Permanent link
Page information