AZ5214 - Basic Process
AZ5214 is a positive PR to start. If you expose and develop, then the exposed areas develop out like a typical positive PR.

However if instead you expose, then post-exposure-Bake “PEB”, the exposed areas become Hardened/impervious to developer. But the rest of the PR is still unexposed.
So THEN you flood expose the rest of the unexposed PR, and like a positive PR this now allows that PR to develop out.

Basic Process Flow
A Basic 5214 the process should look like:
- Spin + soft-bake
- MLA expose
- P.E.Bake - harden the exposed PR, making it "negative"
- Flood expose - expose the remaining positive PR
- Develop