Molecular Vapor Deposition

From UCSB Nanofab Wiki
Revision as of 03:25, 11 May 2018 by John d (talk | contribs) (link to nanoimprint FDTS recipe)
Jump to navigation Jump to search
Molecular Vapor Deposition
Tool Type Vacuum Deposition
Location Bay 4
Supervisor Aidan Hopkins
Supervisor Phone (805) 893-2343
Supervisor E-Mail hopkins@ece.ucsb.edu
Description Molecular Vapor Deposition System
Manufacturer Applied Microstructures Inc.
Vacuum Deposition Recipes


About

The Molecular Vapor deposition system is used for deposition of a monolayer-thick fluorocarbon film for producing extremely hydrophobic surfaces used for anti-sticking layers for nanoimprinting or anti-stiction layers for MEMS. The system has integrated Oxygen plasma cleaning for organic removal and surface activation and can be run at temperatures up to 80°C. Multi-step recipes can be created. The system is currently configured for FDTS (perflourodecyltricholorsilane) and water to producing the coatings. Up to 6” wafers can be coated in the system.

Recipes